MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SK Chemicals SKYTHANE® 194A L series Polyurethane  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP

Material Notes: SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical property. It is widely used for automotive parts and various industrial parts.

Information provided by SK Chemicals

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccASTM D792
Linear Mold Shrinkage 0.0040 cm/cm0.0040 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9696ASTM D2240
Hardness, Shore D 5353ASTM D2240
Tensile Strength, Ultimate 49.0 MPa7110 psiASTM D412
Tensile Stress at Strain  15.7 MPa
@Strain 100 %
2280 psi
@Strain 100 %
ASTM D412
 61.8 MPa
@Strain 300 %
8960 psi
@Strain 300 %
ASTM D412
Elongation at Break 500 %500 %ASTM D412
Resilience 3737by vertical rebound; ASTM D2632
Tear Strength 137 kN/m784 pliDie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 3030H18 Wheel; 1000g load; ASTM D1044
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 130 °C266 °FASTM D1525

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
SK Chemicals SKYTHANE® X595A Polyester Based Thermoplastic Polyurethane Elastomer
SK Chemicals SKYTHANE® S398A Polyester Based Thermoplastic Polyurethane Elastomer
SK Chemicals SKYTHANE® S385A Polyester Based Thermoplastic Polyurethane Elastomer
SK Chemicals SKYTHANE® S195A C series Polyurethane
SK Chemicals SKYTHANE® CS195A Calendaring Series, Polyether Based Thermoplastic Polyurethane Elastomer

PSK089 / 67821

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.