Daelim H&L Plavis N Aromatic Polyimide, Non-Filled, Machined Parts
Categories:
Polymer
;
Thermoset
;
Polyimide, TS
Material Notes:
Superior chemical property, very high radiation resistance, electrical and thermal property, low outgassing and superior physical property
Information provided by Daelim H&L
Key Words:
PI
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.41
g/cc
1.41
g/cc
ASTM D792
Moisture Absorption at Equilibrium
0.95 %
0.95 %
50% RH; ASTM D570
Mechanical Properties
Metric
English
Comments
Hardness, Rockwell M
85 - 100
85 - 100
ASTM D785
Tensile Strength, Ultimate
50.4
MPa
@Temperature 260 °C
7310
psi
@Temperature 500 °F
ASTM D1708
92.1
MPa
@Temperature 23.0 °C
13400
psi
@Temperature 73.4 °F
ASTM D1708
Tensile Strength, Yield
26.4
MPa
@Strain 1 %
3830
psi
@Strain 1 %
ASTM D95
Tensile Stress at Strain
165.1
MPa
@Strain 10 %
23950
psi
@Strain 10 %
ASTM D95
Elongation at Break
8.9 %
@Temperature 260 °C
8.9 %
@Temperature 500 °F
ASTM D1708
12.8 %
@Temperature 23.0 °C
12.8 %
@Temperature 73.4 °F
ASTM D1708
Flexural Strength
65.1
MPa
@Temperature 260 °C
9440
psi
@Temperature 500 °F
ASTM D790
125.6
MPa
@Temperature 23.0 °C
18220
psi
@Temperature 73.4 °F
ASTM D790
Flexural Modulus
1.83
GPa
@Temperature 260 °C
266
ksi
@Temperature 500 °F
ASTM D790
3.1559
GPa
@Temperature 23.0 °C
457.72
ksi
@Temperature 73.4 °F
ASTM D790
Compressive Modulus
2.7213
GPa
@Temperature 23.0 °C
394.69
ksi
@Temperature 73.4 °F
ASTM D695
Shear Strength
90.252
MPa
@Temperature 23.0 °C
13090
psi
@Temperature 73.4 °F
ASTM D732
Izod Impact, Notched (ISO)
5.1012
kJ/m²
2.4278
ft-lb/in²
ASTM D256
Coefficient of Friction
0.24
0.24
Electrical Properties
Metric
English
Comments
Volume Resistivity
1.00e+15
-
1.00e+16
ohm-cm
@Temperature 23.0 °C
1.00e+15
-
1.00e+16
ohm-cm
@Temperature 73.4 °F
ASTM D257
Dissipation Factor
0.0036
@Frequency 1e+6 Hz,
Temperature 23.0 °C
0.0036
@Frequency 1e+6 Hz,
Temperature 73.4 °F
ASTM D150
Thermal Properties
Metric
English
Comments
CTE, linear
5.60
µm/m-°C
@Temperature 23.0 - 260 °C
3.11
µin/in-°F
@Temperature 73.4 - 500 °F
ASTM D696
Specific Heat Capacity
1.17
J/g-°C
0.280
BTU/lb-°F
Decomposition Temperature
616
°C
1140
°F
Oxygen Index
55 %
55 %
ASTM D2863
Descriptive Properties
50% Weight Reduction Time (Minutes)
240
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Manifattura Cattaneo VESPEL® SP1 Polyimide
Daelim H&L Plavis-N ISO Unfilled Aromatic Polyimide Bearing
Daelim H&L Plavis G15 Aromatic Polyimide, 15% Graphite Filled, Machined Parts
Ensinger Sintimid™ V Unfilled Polyimide (PI)
Daelim H&L Plavis-N CM Unfilled Aromatic Polyimide Bearing
PDAEL001 / 82655
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.