MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Crucible Steel REX® M4 High Speed Steel
Categories: Metal; Ferrous Metal; Tool Steel

Material Notes: REX M4 is a special purpose high speed steel designed to give high wear resistance in tools. Its high vanadium and carbon content provide for high resistance to cratering and wear in cold work punches, die inserts, and cutting applications involving high speeds and light cuts. It is designed to give maximum performance working with abrasive materials, exhibiting better wear resistance than M2 or M3.

Information provided by Crucible Industries

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.92 g/cc0.286 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C  63
@Tempering Temp. 568.3 °C
63
@Tempering Temp. 1055 °F
hardened at 2120°F, then quenched and tempered
 65
@Tempering Temp. 551.7 °C
65
@Tempering Temp. 1025 °F
hardened at 2200°F, then quenched and tempered
Modulus of Elasticity 214 GPa31000 ksi
Charpy Impact  11.5 J
@Tempering Temp. 551.7 °C
8.50 ft-lb
@Tempering Temp. 1025 °F
hardened at 2200°F, then tempered; C-notch
 14.9 J
@Tempering Temp. 568.3 °C
11.0 ft-lb
@Tempering Temp. 1055 °F
hardened at 2120°F, then tempered; C-notch
 
Thermal PropertiesMetricEnglishComments
CTE, linear  9.58 µm/m-°C
@Temperature 37.8 - 260 °C
5.32 µin/in-°F
@Temperature 100 - 500 °F
 11.2 µm/m-°C
@Temperature 37.8 - 427 °C
6.24 µin/in-°F
@Temperature 100 - 800 °F
 12.0 µm/m-°C
@Temperature 37.8 - 538 °C
6.64 µin/in-°F
@Temperature 100 - 1000 °F
 12.3 µm/m-°C
@Temperature 37.8 - 649 °C
6.82 µin/in-°F
@Temperature 100 - 1200 °F
 12.6 µm/m-°C
@Temperature 37.8 - 816 °C
6.99 µin/in-°F
@Temperature 100 - 1500 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 840.6 °C1545 °FAc1 Critical Thermal Treatment Temperature
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 1.3 %1.3 %
Chromium, Cr 4.3 %4.3 %
Iron, Fe 79.7 %79.7 %as balance
Manganese, Mn 0.30 %0.30 %
Molybdenum, Mo 4.5 %4.5 %
Silicon, Si 0.30 %0.30 %
Tungsten, W 5.6 %5.6 %
Vanadium, V 4.0 %4.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Crucible Steel CPM® Rex M4 HC(HS) Tool Steel
AISI Type M4 Molybdenum High Speed Tool Steel (UNS T11304)
Bohler-Uddeholm BÖHLER S692/S693 MICROCLEAN® PM M4 High Speed Steel
Carpenter Four Star High Speed Steel Red-Wear® (AISI M4)
Latrobe DuraTech™ M4 Powder Metal High Speed Steel (ASTM M4)

NCRUC906 / 160357

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.