MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Syensqo (Solvay Specialty Polymers) Galden® HT70 PFPE Heat Transfer Fluid
Categories: Fluid; Lubricant; Perfluoropolyether (PFPE)

Material Notes:

Information provided by Solvay

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.68 g/cc0.0607 lb/in³
Solubility in Water 0.0014 %0.0014 %
Kinematic Viscosity 0.50 cSt0.50 cSt
 0.75 cSt
@Temperature 0.000 °C
0.75 cSt
@Temperature 32.0 °F
 1.09 cSt
@Temperature -20.0 °C
1.09 cSt
@Temperature -4.00 °F
 1.79 cSt
@Temperature -40.0 °C
1.79 cSt
@Temperature -40.0 °F
Molecular Weight 410 g/mol410 g/mol
Vapor Pressure 0.188 bar
@Temperature 20.0 °C
141 torr
@Temperature 68.0 °F
Surface Tension 14 dynes/cm14 dynes/cm
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 5.00e+15 ohm-cm5.00e+15 ohm-cm
Dielectric Constant 1.88
@Frequency 1000 Hz
1.88
@Frequency 1000 Hz
Dielectric Strength 15.7 kV/mm399 kV/in2.54 mm gap
Dissipation Factor 0.000200.00020
 
Thermal PropertiesMetricEnglishComments
Heat of Vaporization 71.1 J/g30.6 BTU/lb
CTE, linear 367 µm/m-°C204 µin/in-°Fconverted from volumetric expansion of 0.0011 cm3/cm3-°C
Specific Heat Capacity 0.962 J/g-°C0.230 BTU/lb-°F
Thermal Conductivity 0.0650 W/m-K0.451 BTU-in/hr-ft²-°F
Boiling Point 70.0 °C158 °F
Pour Point -115 °C-175 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.281.28

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Syensqo (Solvay Specialty Polymers) Galden® HT170 PFPE Heat Transfer Fluid
Syensqo (Solvay Specialty Polymers) Galden® LS230 PFPE VPS Fluid
Syensqo (Solvay Specialty Polymers) Galden® HT110 PFPE Heat Transfer Fluid
Syensqo (Solvay Specialty Polymers) Galden® HT230 PFPE Heat Transfer Fluid
Syensqo (Solvay Specialty Polymers) Galden® HT270 PFPE Heat Transfer Fluid

PSOLVAY639 / 218367

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.