MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Clariant Renol PA233HT Nylon 6, Improved Processability, Easily Colorable, Highly Toughened  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes:

Data provided by Clariant Masterbatches

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.07 g/cc1.07 g/ccASTM D792
Water Absorption 1.35 %
@Time 86400 sec
1.35 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.020 cm/cm0.020 in/inASTM D955
Linear Mold Shrinkage, Transverse 0.017 cm/cm0.017 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 47.6 MPa6900 psiASTM D638
Elongation at Break >= 100 %>= 100 %ASTM D638
Elongation at Yield 5.0 %5.0 %ASTM D638
Tensile Modulus 2.17 GPa315 ksiASTM D638
Flexural Yield Strength 77.9 MPa11300 psiASTM D790
Flexural Modulus 2.00 GPa290 ksiASTM D790
Izod Impact, Notched  1.33 J/cm
@Temperature -40.0 °C
2.50 ft-lb/in
@Temperature -40.0 °F
ASTM D256
 8.54 J/cm
@Temperature 22.8 °C
16.0 ft-lb/in
@Temperature 73.0 °F
ASTM D256
Multi-axial Impact @ -30°C Total Energy  62.0 J
@Thickness 12.7 mm
45.7 ft-lb
@Thickness 0.500 in
ASTM D3763
 169 J
@Thickness 25.4 mm
125 ft-lb
@Thickness 1.00 in
ASTM D3763
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 150 °C302 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C131 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Melt Temperature 249 - 277 °C480 - 530 °F
Mold Temperature 65.6 - 79.4 °C150 - 175 °F
Dry Time 2 - 4 hour2 - 4 hourdehumidified dryer
Moisture Content <= 0.20 %<= 0.20 %Processing

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® 8350 HS BK-102 PA6 (Dry)
Adell BD-10 Nylon 6, Ultra High Impact
Ravago Manufacturing Americas Hylon® N2000STHL Nylon 6 (DAM)
Kolon KOPA® KN173HI3R High Impact Nylon 6
Toyobo GLAMIDE® T-779 Nylon-6

PCLAR134 / 82259

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.