MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Latrobe LSS™ H13 PQ Hot Work Tool Steel
Categories: Metal; Ferrous Metal; Alloy Steel; Tool Steel; Hot Work Steel

Material Notes: TLS H13 PQ is Premium Quality H13 hot work steel that is designed to meet the highest quality standards in the die casting industry, and to excel in the most demanding hot work tooling applications. TLS H13 PQ is melted using an electric-arc furnace, is refined by the argon-oxygen-decarburization (AOD) process, and is further enhanced to aerospace quality levels using Vacuum-Arc or Electro-Slag Remelting. These special melting practices along with special thermo-mechanical and annealing treatments result in ultra-high microcleanliness and a homogeneous, fine-grained microstructure.

Information Provided by Timken Latrobe Steel.

Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 7.75 g/cc7.75 g/cc
Density 7.75 g/cc0.280 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 5050Air Cooled from 982°C, 30 minutes
 52.552.5Air Cooled from 1010°C, 30 minutes
 5454Air Cooled from 1032°C, 30 minutes
Modulus of Elasticity 207 GPa30000 ksi
 159 GPa
@Temperature 538 °C
23000 ksi
@Temperature 1000 °F
 186 GPa
@Temperature 204 °C
27000 ksi
@Temperature 400 °F
Machinability 65 - 70 %65 - 70 %1% Carbon Steel
Charpy Impact 13.6 J10.0 ft-lbV-Notch; Air Cooled from 1024°C; 535°C Temper Temperature
 32.5 J24.0 ft-lbV-Notch; Air Cooled from 1024°C; 640°C Temper Temperature
 35.3 J26.0 ft-lbV-Notch; Air Cooled from 1024°C; 260°C Temper Temperature
 
Thermal PropertiesMetricEnglishComments
CTE, linear  11.3 µm/m-°C
@Temperature 21.0 - 204 °C
6.28 µin/in-°F
@Temperature 69.8 - 399 °F
 13.5 µm/m-°C
@Temperature 21.0 - 538 °C
7.50 µin/in-°F
@Temperature 69.8 - 1000 °F
Thermal Conductivity  17.6 W/m-K
@Temperature 27.0 °C
122 BTU-in/hr-ft²-°F
@Temperature 80.6 °F
 23.4 W/m-K
@Temperature 204 °C
162 BTU-in/hr-ft²-°F
@Temperature 399 °F
 26.8 W/m-K
@Temperature 649 °C
186 BTU-in/hr-ft²-°F
@Temperature 1200 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 802 °C1480 °FCritical Temperaure Ar1
 826 °C1520 °FCritical Temperaure Ar3
 840 °C1540 °FCritical Temperaure Ac1
 890 °C1630 °FCritical Temperaure Ac3
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.40 %0.40 %
Chromium, Cr 5.25 %5.25 %
Iron, Fe 90.599 %90.599 %
Manganese, Mn 0.40 %0.40 %
Molybdenum, Mo 1.35 %1.35 %
Silicon, Si 1.0 %1.0 %
Sulfur, S 0.0010 %0.0010 %
Vanadium, V 1.0 %1.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI Type H13 Hot Work Tool Steel
Bohler-Uddeholm UDDEHOLM ORVAR® SUPERIOR (Premium AISI H13) Hot Work Tool Steel
International Mold Steel Premium H13 Hot Work Die and Mold Steel
EDRO #5 H13-Hot Work Tool Steel
Latrobe LSS™ H13 Tool Steel (ASTM H13)

NTIMK084 / 19431

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.