MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC Lexan® 131R PC (Asia Pacific)  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: Nonhalogenated. 3.5 MFR.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccASTM D792
Density 1.19 g/cc0.0430 lb/in³ASTM D792
Water Absorption 0.15 %
@Time 86400 sec
0.15 %
@Time 24.0 hour
ASTM D570
Moisture Absorption at Equilibrium 0.35 %0.35 %ASTM D570
 0.58 %
@Temperature 100 °C
0.58 %
@Temperature 212 °F
ASTM D570
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
0.0050 - 0.0070 in/in
@Thickness 0.126 in
SABIC Method
Melt Flow 3.5 g/10 min
@Load 1.20 kg,
Temperature 300 °C
3.5 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 7070ASTM D785
Hardness, Rockwell R 118118ASTM D785
Tensile Strength at Break 65.0 MPa9430 psiType I, 50 mm/min; ASTM D638
Tensile Strength, Yield 62.0 MPa8990 psiType I, 50 mm/min; ASTM D638
Elongation at Break 110 %110 %Type I, 50 mm/min; ASTM D638
Elongation at Yield 7.0 %7.0 %Type I, 50 mm/min; ASTM D638
Flexural Yield Strength 93.0 MPa13500 psi1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.34 GPa339 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 9.07 J/cm17.0 ft-lb/inASTM D256
Izod Impact, Unnotched 32.04 J/cm60.02 ft-lb/inASTM D4812
Tensile Impact Strength 546 kJ/m²260 ft-lb/in²Type S; ASTM D1822
Dart Drop, Total Energy 169 J125 ft-lbASTM D3029
Taber Abrasion, mg/1000 Cycles 1010CS-17, 1 kg; ASTM D1044
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+17 ohm-cm>= 1.00e+17 ohm-cmASTM D257
Dielectric Constant  2.96
@Frequency 1e+6 Hz
2.96
@Frequency 1e+6 Hz
ASTM D150
 3.17
@Frequency 50.0 - 60.0 Hz
3.17
@Frequency 50.0 - 60.0 Hz
ASTM D150
Dielectric Strength 15.0 kV/mm
@Thickness 3.20 mm
381 kV/in
@Thickness 0.126 in
in air; ASTM D149
Dissipation Factor  0.00090
@Frequency 50.0 - 60.0 Hz
0.00090
@Frequency 50.0 - 60.0 Hz
ASTM D150
 0.010
@Frequency 1e+6 Hz
0.010
@Frequency 1e+6 Hz
ASTM D150
Comparative Tracking Index 250 - 400 V250 - 400 VUL 746A
Hot Wire Ignition, HWI 30 - 60 sec30 - 60 secUL 746A
High Amp Arc Ignition, HAI 60 - 120 arcs60 - 120 arcsUL 746A
High Voltage Arc-Tracking Rate, HVTR 25.4 - 80.0 mm/min1.00 - 3.15 in/minUL 746A
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 68.4 µm/m-°C
@Temperature -40.0 - 95.0 °C
38.0 µin/in-°F
@Temperature -40.0 - 203 °F
ASTM E 831
Specific Heat Capacity 1.26 J/g-°C0.301 BTU/lb-°FASTM C351
Thermal Conductivity 0.190 W/m-K1.32 BTU-in/hr-ft²-°FASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 137 °C
@Thickness 6.40 mm
279 °F
@Thickness 0.252 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 132 °C
@Thickness 6.40 mm
270 °F
@Thickness 0.252 in
unannealed; ASTM D648
Vicat Softening Point 154 °C309 °FRate B/50; ASTM D1525
UL RTI, Electrical 125 °C257 °FUL 746B
UL RTI, Mechanical with Impact 115 °C239 °FUL 746B
UL RTI, Mechanical without Impact 125 °C257 °FUL 746B
Flammability, UL94 HB
@Thickness 1.47 mm
HB
@Thickness 0.0579 in
UL 94
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.5861.586ASTM D542
Haze 1.0 %
@Thickness 2.54 mm
1.0 %
@Thickness 0.100 in
ASTM D1003
Transmission, Visible 88 %88 %2.54 mm; ASTM D1003
 
Descriptive Properties
Specific Volume0.83cm^3/gASTM D792
UV-light, water exposure/immersionF2UL 746C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trinseo CALIBRE™ 603-3 Polycarbonate, Branched

PSABI53177 / 153223

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.