MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lubrizol ESTANE® 58137 Ester Based Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Polyester Grade

Material Notes: Features: Fast cycling, broad temperature performance, and durability

Use: Injection Molding

Available in Americas, Europe, Middle East, Africa, India and Asia

Information provided by Lubrizol.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.24 g/cc1.24 g/ccASTM D792
Maximum Moisture Content 0.0200.020
Linear Mold Shrinkage 0.0080 cm/cm0.0080 in/inflex bar, Injection
 0.0090 cm/cm0.0090 in/indisk, Injection
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 62 - 68
@Time 5.00 sec
62 - 68
@Time 0.00139 hour
ASTM D2240
Tensile Strength 41.0 MPa5950 psiASTM D412
Elongation at Break 430 %430 %ASTM D412
100% Modulus 21.0 MPa
@Strain 100 %
3050 psi
@Strain 100 %
ASTM D412
300% Modulus 31.0 MPa
@Strain 300 %
4500 psi
@Strain 300 %
ASTM D412
Flexural Modulus 0.372 GPa54.0 ksiASTM D790
Tear Strength 50.8 kN/m290 pliADM D470
Graves Tear Strength 210 kN/m1200 pliDie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 1919CS-17, 1000g; ASTM D3389 B
Compression Set  42 %
@Temperature 23.0 °C,
Time 79200 sec
42 %
@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395
 61 %
@Temperature 70.0 °C,
Time 79200 sec
61 %
@Temperature 158 °F,
Time 22.0 hour
ASTM D395
 
Thermal PropertiesMetricEnglishComments
Melting Point 227 °C441 °FDSC
Glass Transition Temp, Tg -15.0 °C5.00 °FDSC
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 210 °C410 °FInjection
Middle Barrel Temperature 221 °C430 °FInjection
Front Barrel Temperature 229 °C444 °FInjection
Nozzle Temperature 232 °C450 °FInjection
Melt Temperature 232 °C450 °FInjection
Drying Temperature 104 °C219 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour
Dew Point -40.0 °C-40.0 °F
Back Pressure >= 50.0 MPa>= 7250 psiInjection
Screw Speed 60 - 100 rpm60 - 100 rpmInjection

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Zytel® ST801 NC010A PA66-HI
Envalior Stanyl® TW441 Nylon 46 (European and Asian Grade) (Dry)
Lubrizol ESTANE® 58133 Ester Based Thermoplastic Polyurethane
Celanese Zytel® 151L NC010 PA612
Celanese Celstran® TPU-GF40-01-US TPU, 40% Glass Reinforced

PNOVEON025 / 55291

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.