MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Phosphor bronze 10% Sn, UNS C52400, H06 Temper flat products
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: Good to excellent corrosion resistance. Good cold workability for blanking, forming and bending, shearing.

Applications: heavy bars and plates for severe compression, bridge and expansion plates and fittings, articles requiring good spring qualities, resiliency, fatigue resistance, good wear and corrosion resistance.

Trace content of Phosphorus.

Test specimen: flat products - 1mm thickness.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.78 g/cc0.317 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 100100
Tensile Strength, Ultimate 795 MPa115000 psi
Elongation at Break 7.0 %7.0 %In 50 mm
Modulus of Elasticity 110 GPa16000 ksi
Poissons Ratio 0.3410.341
Machinability 30 %30 %UNS C36000 (free-cutting brass) = 100%
Shear Modulus 41.0 GPa5950 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000157 ohm-cm
@Temperature 20.0 °C
0.0000157 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 18.4 µm/m-°C
@Temperature 20.0 - 300 °C
10.2 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.380 J/g-°C0.0908 BTU/lb-°F
Thermal Conductivity 50.0 W/m-K
@Temperature 20.0 °C
347 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point 845 - 1000 °C1550 - 1830 °F
Solidus 845 °C1550 °F
Liquidus 1000 °C1830 °F
Annealing Point 482 - 677 °C900 - 1250 °F
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 475 - 675 °C887 - 1250 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 88.3 - 90.07 %88.3 - 90.07 %
Iron, Fe <= 0.10 %<= 0.10 %
Lead, Pb <= 0.050 %<= 0.050 %
Phosphorus, P 0.030 - 0.35 %0.030 - 0.35 %
Tin, Sn 9.0 - 11 %9.0 - 11 %
Zinc, Zn <= 0.20 %<= 0.20 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Phosphor bronze 10% Sn, UNS C52400, H02 Temper flat products
Phosphor bronze 5% Sn, UNS C51000
Phosphor bronze 10% Sn, UNS C52400, H04 Temper flat products
Phosphor bronze 10% Sn, UNS C52400, H08 Temper flat products
Phosphor bronze 10% Sn, UNS C52400, H10 Temper flat products

MC52400b6 / 11554

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.