MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 1500.5-55D Polyether-Ester Block Copolymer (TEEE/COPE), Glass Fiber
Categories: Polymer; Thermoplastic; Polyester, TP

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.22 g/cc1.22 g/ccASTM D 792
Filler Content 5 %5 %Primary Additive
Water Absorption 0.40 %0.40 %24 hrs @ 23°C; ASTM D 570
Linear Mold Shrinkage 0.0050 - 0.0090 cm/cm
@Thickness 3.17 mm
0.0050 - 0.0090 in/in
@Thickness 0.125 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5555instantaneous; ASTM D 2240
Tensile Strength at Break 28.58 MPa4145 psiASTM D 638
Elongation at Break 500 %500 %ASTM D 638
Tensile Modulus 0.552 GPa80.0 ksiASTM D 638
Flexural Strength 17.7 MPa2570 psiASTM D 790
Flexural Modulus 0.414 GPa60.0 ksiASTM D 790
Izod Impact, Notched 4.16 J/cm
@Thickness 3.17 mm
7.80 ft-lb/in
@Thickness 0.125 in
D 256
Izod Impact, Unnotched 5.66 J/cm
@Thickness 3.17 mm
10.6 ft-lb/in
@Thickness 0.125 in
ASTM D4812
 
Processing PropertiesMetricEnglishComments
Melt Temperature 210 - 238 °C410 - 460 °F
Mold Temperature 21.1 - 37.8 °C70.0 - 100 °F
Drying Temperature 104 °C220 °F
Dry Time 2 - 4 hour2 - 4 hour
Moisture Content <= 0.10 %<= 0.10 %
Injection Pressure 68.9 - 103 MPa10000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow PELLETHANE® 2104-45D Polyurethane Elastomer (Ether-Ether Hybrid)
Covestro Desmopan® 9868DU Polyurethane
Celanese Zytel® ST801 NC010A PA66-HI
Celanese Vandar® AB700 High Modulus Polyester Alloy
Celanese SO.F.TER Pibiflex® 6097 NERO Copolyester TPE

PQZWA2415 / 91132

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.