MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Schott N-LAF34 Glass
Categories: Ceramic; Glass

Material Notes:

Information Provided by SCHOTT North America, Inc.

Key Words: 773496.424
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 4.24 g/cc0.153 lb/in³
 
Chemical PropertiesMetricEnglishComments
Acid Class, SR 51.351.3
Alkali Class, AR 1.01.0
Stain Resistance Class, FR 1.01.0
 
Mechanical PropertiesMetricEnglishComments
Knoop Microhardness 770770.1/20
Modulus of Elasticity 123 GPa17800 ksi
Poissons Ratio 0.2920.292
Shear Modulus 48.0 GPa6960 ksicalculated
 
Thermal PropertiesMetricEnglishComments
CTE, linear  5.80 µm/m-°C
@Temperature -30.0 - 70.0 °C
3.22 µin/in-°F
@Temperature -22.0 - 158 °F
 7.00 µm/m-°C
@Temperature 20.0 - 300 °C
3.89 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.800 J/g-°C0.191 BTU/lb-°F
Thermal Conductivity 0.560 W/m-K3.89 BTU-in/hr-ft²-°F
Transformation Temperature, Tg 668 °C1230 °F
Softening Point 745 °C1370 °FViscosity 107.6 dPa s
Annealing Point 659 °C1220 °FViscosity 1013.0 dPa s
 
Optical PropertiesMetricEnglishComments
Refractive Index  1.7725
@Wavelength 587.6 nm
1.7725
@Wavelength 587.6 nm
nd
 1.77621
@Wavelength 546.1 nm
1.77621
@Wavelength 546.1 nm
ne
Abbe Number 49.3849.38ve
 49.6249.62vd
Optical Dispersion 0.0155680.015568nf - nc
 0.0157190.015719nf' - nc'
Transmission, Visible  91.9 %
@Thickness 10.0 mm,
Wavelength 380 nm
91.9 %
@Thickness 0.394 in,
Wavelength 380 nm
 97.1 %
@Thickness 10.0 mm,
Wavelength 405 nm
97.1 %
@Thickness 0.394 in,
Wavelength 405 nm
 99.2 %
@Thickness 10.0 mm,
Wavelength 460 nm
99.2 %
@Thickness 0.394 in,
Wavelength 460 nm
 99.8 %
@Thickness 10.0 mm,
Wavelength 580 nm
99.8 %
@Thickness 0.394 in,
Wavelength 580 nm
 99.8 %
@Thickness 10.0 mm,
Wavelength 700 nm
99.8 %
@Thickness 0.394 in,
Wavelength 700 nm
IR Transmittance  44.2 %
@Thickness 10.0 mm,
Wavelength 2500 nm
44.2 %
@Thickness 0.394 in,
Wavelength 2500 nm
 99 %
@Thickness 10.0 mm,
Wavelength 1530 nm
99 %
@Thickness 0.394 in,
Wavelength 1530 nm
UV Transmittance  1.0 %
@Thickness 10.0 mm,
Wavelength 320 nm
1.0 %
@Thickness 0.394 in,
Wavelength 320 nm
 25 %
@Thickness 10.0 mm,
Wavelength 334 nm
25 %
@Thickness 0.394 in,
Wavelength 334 nm
 63.4 %
@Thickness 10.0 mm,
Wavelength 350 nm
63.4 %
@Thickness 0.394 in,
Wavelength 350 nm
 86.7 %
@Thickness 10.0 mm,
Wavelength 370 nm
86.7 %
@Thickness 0.394 in,
Wavelength 370 nm
 
Descriptive Properties
B0
Climatic Resistance Test CR1
HG2
K (10-6mm2/N)1.44
Phosphate Resistance PR1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Schott SF56A Glass
Solvay Thornel® Mat VMC Carbon Fiber
Schott N-LAF36 Glass
Schott N-LAF35 Glass
Schott N-LAF21 Glass

CSGS057 / 93391

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.