MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

NuSil MED2-4213 Silicone, Two part Adhesive - Unrestricted Medical Use
Categories: Polymer; Adhesive; Thermoset; Silicone

Material Notes: Description: Silicone adhesives are elastomers or pressure sensitive adhesive systems that are designed to bond silicone surfaces to each other and to other substrate surfaces such as metals and plastics. There are one-part and two-part adhesives, ranging in consistency from flowable to non-flowable (non-slump). Silicone primers are specially formulated silanes supplied in a solvent that are used to improve the bond strength between a silicone elastomer or adhesive and another substrate surface (silicone, metals, and certain plastics).

Important Properties of Adhesives: In general, silicone adhesives adhere well to substrates such as glass, aluminum, titanium, other silicones, and some ceramics. While various types of materials can be used as adhesives, silicones are consistently chosen for their many inherent properties and overall versatility. Advantages of these adhesives are as versatile as silicone itself:

  • Proven biocompatibility
  • Resistance to moisture
  • Ability to remain elastic at temperatures below 0 ºC
  • Ability to resist chemical breakdown at temperatures >200 ºC
  • Low modulus prevents warpage, delamination and substrate failure.
Comments: HTV, Fast Cure, High Extrusion Rate

Cure System: Platinum

Information provided by NuSil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.12 g/cc1.12 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 1212Certified
 1515Typical
Tensile Strength at Break 3.80 MPa551 psiCertified
 6.90 MPa1000 psiTypical
Elongation at Break 600 %600 %Certified
 800 %800 %Typical
Tear Strength 10.5 kN/m60.0 pliCertified
 22.8 kN/m130 pliTypical
 
Processing PropertiesMetricEnglishComments
Cure Time 15.0 min
@Temperature 150 °C
0.250 hour
@Temperature 302 °F
Working Life 900 min
@Temperature 25.0 °C
900 min
@Temperature 77.0 °F
 
Descriptive Properties
Mix Ratio1:1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
NuSil MED-4910 Liquid Silicone Rubber - Restricted Medical Use
NuSil MED-4014 Silicone, Two Part High Consistency Elastomer - Restricted Medical Use
NuSil LSR-5810 Liquid Silicone Rubbers (LSR)
ELASTO UK Dryflex® 8006-101 Flame Retardant TPE for Injection Molding, Black, Halogen Free
Polymax® Maxelast® C4912 TPE, Transparent

PNUSIL274 / 141998

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.