MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Trinseo EMERGE™ PC/PET 9100CR MED Polycarbonate Resin
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/PET Polyester Blend

Material Notes: EMERGE™ PC/PET 9100CR advanced resin is a polycarbonate blend with excellent chemical resistance. This grade was designed for use in medical equipment housings and can withstand repeated exposure to a variety of cleaners and disinfectants commonly used in hospitals. This grade has good aesthetics and excellent toughness.

Main Characteristics:

  • Excellent chemical resistance
  • Tested under ISO 10993
  • UL listing for HB
Applications:
  • Medical device housings or enclosures

Information provided by Trinseo.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.23 g/cc0.0444 lb/in³ASTM D792
Linear Mold Shrinkage, Flow 0.0060 - 0.0090 cm/cm0.0060 - 0.0090 in/inASTM D955
Linear Mold Shrinkage, Transverse 0.0050 - 0.0080 cm/cm0.0050 - 0.0080 in/inASTM D955
Melt Flow 8.5 g/10 min
@Load 5.00 kg,
Temperature 260 °C
8.5 g/10 min
@Load 11.0 lb,
Temperature 500 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 111
@Thickness 3.20 mm
111
@Thickness 0.126 in
Injection Molded; ASTM D785
Tensile Strength at Break 56.2 MPa
@Thickness 3.20 mm
8150 psi
@Thickness 0.126 in
Injection Molded, 50 mm/min; ASTM D638
Tensile Strength, Yield 50.0 MPa
@Thickness 3.20 mm
7250 psi
@Thickness 0.126 in
Injection Molded, 50 mm/min; ASTM D638
Elongation at Break 150 %
@Thickness 3.20 mm
150 %
@Thickness 0.126 in
Injection Molded, 50 mm/min; ASTM D638
Elongation at Yield 4.7 %
@Thickness 3.20 mm
4.7 %
@Thickness 0.126 in
Injection Molded, 50 mm/min; ASTM D638
Tensile Modulus 2.21 GPa
@Thickness 3.20 mm
321 ksi
@Thickness 0.126 in
Injection Molded, 5.0 mm/min; ASTM D638
Flexural Strength 77.2 MPa
@Thickness 3.20 mm
11200 psi
@Thickness 0.126 in
Injection Molded, 1.3 mm/min; ASTM D790
Flexural Modulus 2.10 GPa305 ksiInjection Molded, 1.3 mm/min; ASTM D790
Izod Impact, Notched  7.50 J/cm
@Temperature -30.0 °C
14.1 ft-lb/in
@Temperature -22.0 °F
Injection Molded; ASTM D256
 9.10 J/cm
@Temperature 23.0 °C
17.0 ft-lb/in
@Temperature 73.4 °F
Injection Molded; ASTM D256
Dart Drop, Total Energy  46.3 J
@Thickness 3.20 mm,
Temperature 23.0 °C
34.1 ft-lb
@Thickness 0.126 in,
Temperature 73.4 °F
Injection Molded, Peak Energy; ASTM D3763
 55.4 J
@Thickness 3.20 mm,
Temperature -40.0 °C
40.9 ft-lb
@Thickness 0.126 in,
Temperature -40.0 °F
Injection Molded, Peak Energy; ASTM D3763
 63.3 J
@Thickness 3.20 mm,
Temperature 23.0 °C
46.7 ft-lb
@Thickness 0.126 in,
Temperature 73.4 °F
Injection Molded; ASTM D3763
 80.2 J
@Thickness 3.20 mm,
Temperature -40.0 °C
59.2 ft-lb
@Thickness 0.126 in,
Temperature -40.0 °F
Injection Molded; ASTM D3763
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 3.40e+15 ohm-cm3.40e+15 ohm-cmIEC 60093
Surface Resistance 4.30e+15 ohm4.30e+15 ohmIEC 60093
Dielectric Constant  3.12
@Frequency 1e+6 Hz
3.12
@Frequency 1e+6 Hz
IEC 60250
 3.28
@Frequency 100 Hz
3.28
@Frequency 100 Hz
IEC 60250
Dielectric Strength  17.0 kV/mm
@Thickness 3.20 mm
432 kV/in
@Thickness 0.126 in
in Oil; IEC 60243-1
 28.0 kV/mm
@Thickness 1.60 mm
711 kV/in
@Thickness 0.0630 in
in Oil; IEC 60243-1
Dissipation Factor  0.0020
@Frequency 100 Hz
0.0020
@Frequency 100 Hz
IEC 60250
 0.020
@Frequency 1e+6 Hz
0.020
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 117 °C243 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 87.2 °C189 °FUnannealed; ASTM D648
Vicat Softening Point 144 °C291 °FRate B (120°C/h), Loading 2 (10 N); ASTM D1525
Flammability, UL94 HB
@Thickness 1.00 mm
HB
@Thickness 0.0394 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 249 - 282 °C480 - 540 °F
Mold Temperature 43.0 - 99.0 °C109 - 210 °F
Drying Temperature 121 °C250 °F
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trinseo EMERGE™ PC/ABS 7100 MED Polycarbonate Resin
Trinseo EMERGE™ 7100 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS)
Envalior Arnite® T06 202 /A PBT
Envalior Arnitel® PM471 TPC-ET, Injection Molding
INEOS Styrolution Terlux® 2802 Transparent MABS

PTRINS9056 / 197552

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.