MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Moplen RP346R Polypropylene Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Moplen RP346R is a medium flow polypropylene random copolymer resin, with high clarity, excellent flowability, good stiffness impact balance, good dimensional stability. Typical customer applications are thin wall food packaging, clear ISBM bottles, food and household containers and boxes, furniture. Applications: Bottles For Consumer Goods, Caps & Closures, Clear Containers, Containers, Furniture, House wares, TWIM Food Containers.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ASTM D792
Melt Flow 25 g/10 min
@Load 2.16 kg,
Temperature 230 °C
25 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 29.0 MPa4210 psiASTM D882
Elongation at Yield 13 %13 %ASTM D638
Flexural Modulus 1.05 GPa152 ksiASTM D790
Izod Impact, Notched 0.500 J/cm
@Temperature 23.0 °C
0.937 ft-lb/in
@Temperature 73.4 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C185 °FASTM D648
 
Descriptive Properties
Processing MethodInjection blow Molding, injection molding, injection stretch blow molding

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Moplen RP344RK Polypropylene Copolymer
LyondellBasell Moplen RP2380 Polypropylene Copolymer
LyondellBasell Moplen RP2965 Polypropylene Copolymer
LyondellBasell Moplen RP344NK Polypropylene Copolymer
Formosa Plastics Formolene® 2306N Impact Copolymer Polypropylene

PEQT9104 / 220735

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.