MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Borealis FT5236 Low Density Polyethylene
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: FT5236 is a Low Density Polyethylene for Film Extrusion. Tubular Technology. Includes anti-block, antioxidant and medium slip additives. Applications FT5236 has been developed especially for applications like: carrier-bag film, pouches, lamination films, and food packaging.

Information provided by Borealis AG

Key Words: LDPE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.923 g/cc0.0333 lb/in³ISO 1183
Melt Flow 0.75 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.75 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Antiblock Level 800 ppm800 ppmsynthetic silica; Borealis Method
Slip Level 550 ppm550 ppmerucamide; Borealis Method
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 250 %250 %ISO 527-3
Film Elongation at Break, TD 550 %550 %ISO 527-3
Tensile Modulus 0.230 GPa33.4 ksiMD; ASTM D882-A
 0.260 GPa37.7 ksiTD; ASTM D882-A
Puncture Energy 2.50 J1.84 ft-lb66N; ASTM D5748
Coefficient of Friction, Dynamic 0.200.20ISO 8295
Elmendorf Tear Strength, MD 10.19 g/micron258.8 g/milISO 6383/2
Elmendorf Tear Strength, TD 5.097 g/micron129.5 g/milISO 6383/2
Dart Drop Test 120 g
@Thickness 0.0400 mm
0.265 lb
@Thickness 0.00157 in
ISO 7765-1
Film Tensile Strength at Break, MD 27.0 MPa3920 psiISO 527-3
Film Tensile Strength at Break, TD 24.0 MPa3480 psiISO 527-3
 
Thermal PropertiesMetricEnglishComments
Melting Point 112 °C234 °FISO 11357-3
Vicat Softening Point 97.0 °C207 °FISO 306
 
Optical PropertiesMetricEnglishComments
Haze 8.0 %8.0 %ASTM D1003
Gloss 85 %85 %ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis FG5224 Linear Low Density Polyethylene
Borealis FT3200 Low Density Polyethylene
Borealis HD234CF Polypropylene
Borealis FS1470 High Density Polyethylene
Borealis FT5230 Low Density Polyethylene

PBOREA456 / 108715

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.