MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow Engage® 8130 Polyolefin Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Elastomer, Melt-Processible Rubber

Material Notes: Description: Engage® 8130 polyolefin elastomer is an ethyleneoctene copolymer with low density and a high melt index. This combination provides excellent toughness, flexibility, and ease in processing and makes Engage® 8130 highly effective as an impact modifier in polyolefins or as a component in injection molding applications. The product form is free-flowing pellets.

Information provided by manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.864 g/cc0.0312 lb/in³ASTM D792
Mooney Viscosity 5.8
@Temperature 100 °C
5.8
@Temperature 212 °F
ML 1 + 4; ASTM D1646
Melt Index of Compound 13 g/10 min
@Load 2.16 kg,
Temperature 190 °C
13 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6060ASTM D2240
Tensile Strength, Ultimate 2.00 MPa290 psi508 mm/min; ASTM D638
Tensile Strength, Yield 1.90 MPa276 psi508 mm/min; ASTM D638
Elongation at Break 760 %760 %508 mm/min; ASTM D638
2% Secant Modulus 0.00690 GPa1.00 ksiASTM D790
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature <= -76.0 °C<= -105 °FASTM D746
 
Descriptive Properties
Comonomer Content42 wt%Dow Method (13C NMR/FTIR)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow Engage® 8150 Polyolefin Elastomer
Dow Engage® 8200 Polyolefin Elastomer
Dow Engage® 8400 Polyolefin Elastomer
Dow Engage® 8107 Polyolefin Elastomer
Dow Engage® 8407 Polyolefin Elastomer

PDVE29 / 34080

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.