MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Teknor Apex Elexar® EL 1446A Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Elexar® is a family of styrene block copolymer thermoplastic elastomers, often referred to as thermoplastic rubber (TPR). Elexar® "rubber-like" compounds offer superior electrical properties coupled with excellent flexibility, toughness, and surface aesthetics. Elexar® compounds are specially designed for wire & cable, fiber optic, and electrical/electronics. Elexar® TPEs are excellent alternatives to thermoset rubber, TPU's, and flexible PVC. RoHS Compliant

Uses: Insulation; Jacketing

Wire Types: SEOW FR

Information Provided by Teknor Apex

Key Words: TPE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.25 g/cc1.25 g/cc
Melt Flow 18 g/10 min
@Load 5.00 kg,
Temperature 200 °C
18 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 3737
Tensile Strength 11.0 MPa1600 psi
Elongation at Break 600 %600 %
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94 V-0V-0
Oxygen Index 27 %27 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Teknor Apex ELEXAR® EL 8730 Thermoplastic Elastomer
RTP Company RTP 2800B-80A HF  Thermoplastic Vulcanizate Elastomer (TPV) 80 Shore A - High Flow
Teknor Apex Elexar® EL 1934D Thermoplastic Elastomer
Huntsman IROGRAN® A 85 P 4934 Ether-Based TPU-For Cable Industry
Teknor Apex Monprene® MP 1304 Thermoplastic Elastomer

PTEKNO784 / 128965

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.