MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chi Mei Kibisan® PN-117 SAN  (discontinued **)
Categories: Polymer; Thermoplastic; SAN Polymer; Styrene Acrylonitrile (SAN), Molded

Material Notes: Injection Molding

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.06 g/cc0.0383 lb/in³ISO 1183
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm0.0020 - 0.0040 in/inASTM D955
Melt Flow  2.8 g/10 min
@Load 5.00 kg,
Temperature 200 °C
2.8 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 14 g/10 min
@Load 3.80 kg,
Temperature 230 °C
14 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
 32 g/10 min
@Load 10.0 kg,
Temperature 220 °C
32 g/10 min
@Load 22.0 lb,
Temperature 428 °F
Melt Volume Rate (ml/10 min); ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 8383ASTM D790
Ball Indentation Hardness 159 MPa23100 psiH358/30; ISO 2039-1
Tensile Strength at Break 64.0 MPa9280 psi50 mm/min; ISO 527
Tensile Strength, Yield 68.0 MPa9860 psi50 mm/min; ISO 527
 69.36 MPa
@Thickness 3.17 mm
10060 psi
@Thickness 0.125 in
ASTM D638
Elongation at Break 6.0 %6.0 %50 mm/min; ISO 527
Flexural Strength 93.0 MPa13500 psi2 mm/min; ISO 178
Flexural Yield Strength 97.9 MPa
@Thickness 3.17 mm
14200 psi
@Thickness 0.125 in
ASTM D790
Flexural Modulus 2.70 GPa392 ksi2 mm/min; ISO 178
Izod Impact, Notched  0.166 J/cm
@Thickness 6.35 mm,
Temperature 23.0 °C
0.310 ft-lb/in
@Thickness 0.250 in,
Temperature 73.4 °F
ASTM D256
 0.176 J/cm
@Thickness 3.17 mm,
Temperature 23.0 °C
0.330 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Izod Impact, Notched (ISO) 3.00 kJ/m²1.43 ft-lb/in²ISO 180/1A
Izod Impact, Unnotched (ISO) 15.0 kJ/m²7.14 ft-lb/in²ISO 180/1C
Charpy Impact Unnotched 2.00 J/cm²9.52 ft-lb/in²ISO 179
Charpy Impact, Notched 0.200 J/cm²0.952 ft-lb/in²ISO 179
Impact 3.03.0Impact Flexural Test Notched (KJ/m²)
 1919Impact Flexural Test Unnotched (KJ/m²)
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 86.0 °C187 °Funannealed; ISO 75
 97.0 °C207 °Fannealed; ISO 75
Vicat Softening Point  102 °C
@Load 5.00 kg
216 °F
@Load 11.0 lb
50°C/hr; ISO 306
 104 °C
@Load 5.00 kg
219 °F
@Load 11.0 lb
120°C/hr; ISO 306
 106 °C
@Load 1.00 kg
223 °F
@Load 2.20 lb
50°C/hr; ISO 306
 109 °C
@Load 1.00 kg
228 °F
@Load 2.20 lb
120°C/hr; ISO 306
Flammability, UL94  HB
@Thickness 1.59 mm
HB
@Thickness 0.0625 in
 HB
@Thickness 1.59 mm
HB
@Thickness 0.0625 in
UL 94

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chi Mei Kibisan® PN-127 SAN
Chi Mei Kibisan® PN-107 L125 SAN
INEOS Styrolution Luran® HH-120 Alpha-Methylstyrene Acrylonitrile
Chi Mei Kibisan® PN-106 L150 SAN
Chi Mei Kibisan® PN137H SAN Resin, General Purpose

PCHI975 / 109463

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.