MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Denka MALECCA K-600 ABS
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: A heat-resistant ABS resin based on "DENKA IP" – a Styrene-N-Phenylmaleimide copolymer. It has been designed as an easy-to-use resin by improving conventional heat-resistant ABS resins which had defects in terms of moldability, thermal stability, and impact resistance.

Applications

  • Mobile phones
  • vehicle-mounted audio equipment
  • automotive interior components
  • home electric appliances
  • OA equipment, etc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.07 g/cc1.07 g/ccASTM D792
Density 1.07 g/cc0.0387 lb/in³ISO 1183
Melt Flow 15 g/10 min
@Load 10.0 kg,
Temperature 265 °C
15 g/10 min
@Load 22.0 lb,
Temperature 509 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 111111ISO 2039-2
 117117ASTM D785
Tensile Strength at Break 37.0 MPa5370 psi50mm/min; ISO 527-2
 39.0 MPa5660 psiASTM D638
Tensile Strength, Yield 37.0 MPa5370 psiISO 527-2
Elongation at Break 26 %26 %ISO 527-2
Tensile Modulus 2.10 GPa305 ksi1mm/min; ISO 527-1
Flexural Strength 64.0 MPa9280 psi15mm/min; ASTM D790
 67.0 MPa9720 psiISO 178
Flexural Modulus 1.95 GPa283 ksi15mm/min; ASTM D790
 2.05 GPa297 ksi2mm/min; ISO 178
Izod Impact, Notched 1.46 J/cm
@Temperature 23.0 °C
2.74 ft-lb/in
@Temperature 73.4 °F
ASTM D256
Charpy Impact, Notched 1.30 J/cm²6.19 ft-lb/in²ISO 179-2
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 112 °C234 °FISO 75-2
 122 °C252 °FASTM D648
Vicat Softening Point 133 °C271 °F50N; ISO 306
Flammability, UL94 HBHB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Denka MALECCA K-300 ABS
Elix Polymers ELIX ABS H605 Acrylonitrile Butadiene Styrene (ABS), Heat Resistant
Clariant Renol ABS3470 ABS, High Heat, Low Gloss
Chi Mei Polylac® PA-777B ABS - High Heat
Chi Mei Polylac® PA-747 ABS

PDENK008 / 29672

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.