MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chemours Krytox® XHT-BDX Performance PFPE Lubricant
Categories: Fluid; Lubricant; Perfluoropolyether (PFPE)

Material Notes: Extreme high temperature PFPE Grease with non-melting thickener and low evaporation. Easily wets metallic surfaces.

Chemours was formed from former DuPont performance chemicals businesses, including DuPont Performance Lubricants, in 2015.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.00 g/cc
@Temperature 0.000 °C
2.00 g/cc
@Temperature 32.0 °F
Volatiles 1.5 %
@Temperature 260 °C,
Time 79200 sec
1.5 %
@Temperature 500 °F,
Time 22.0 hour
Oil Volatility; ASTM D2595
Kinematic Viscosity 2610 cSt
@Temperature 20.0 °C
2610 cSt
@Temperature 68.0 °F
Base Oil
Kinematic Viscosity at 40°C (104°F) 738 cSt738 cStBase Oil
Kinematic Viscosity at 100°C (212°F) 65 cSt65 cStBase Oil
Vapor Pressure  <= 4.00e-17 bar
@Temperature 20.0 °C
<= 3.00e-14 torr
@Temperature 68.0 °F
 <= 1.33e-12 bar
@Temperature 100 °C
<= 1.00e-9 torr
@Temperature 212 °F
 <= 2.67e-9 bar
@Temperature 200 °C
<= 0.00000200 torr
@Temperature 392 °F
 
Mechanical PropertiesMetricEnglishComments
Oil Separation 5.0 %
@Temperature 99.0 °C,
Time 108000 sec
5.0 %
@Temperature 210 °F,
Time 30.0 hour
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 350 °C662 °F
 400 °C752 °Fintermittent spikes
Minimum Service Temperature, Air <= -15.0 °C<= 5.00 °F
Pour Point <= -20.0 °C<= -4.00 °FBase Oil
 
Descriptive Properties
AppearanceWhite, creamy consistency
Standard NLGI Penetration Grade1.5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chemours Krytox® 205 GPL Standard Grade Grease
Aluminum A201.0 Composition Spec
A286 IRON BASED 15Cr-26Ni-1.3Mo-2.1Ti-0.3V SUPERALLOY FORGINGS FOR GAS TURBINE DISCS
Special Metals INCONEL® Alloy 625
Chemours Krytox® NRT 8904 PFPE Lubricant

WDUPJ922 / 162456

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.