MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Solvay Chemicals CASO® FCC FLAKES Food Additive INS 509, Calcium Chloride
Categories: Ceramic; Halide

Material Notes: CASO® FCC Flakes is a dihydrate calcium chloride food grade of mineral origin. According to the International Numbering System (INS) for food additives, CASO® FCC Flakes is characterized by the INS Number 509 referring to "calcium chloride". CASO® FCC Flakes is compatible with the food uses for which the Food Chemicals Codex (8th Edition) specifications are required, but does not constitute a food additive pursuant to European Regulation N° 1333/2008 as amended.

REACH Registration Number: 01-2119494219-28/ CAS number: 10035-04-8/ EINECS - N°: 233-140-8/ CE - N°: 017-013-00-2

Applications: Agriculture, Dairy products and cheese, Production of beer and soft drinks, Storage of canned fruits and vegetables, Cooling agent in food processes and Food Additive

Information provided by Solvay

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.800 - 0.900 g/cc0.0289 - 0.0325 lb/in³
Molecular Weight 147.02 g/mol147.02 g/mol
 
Descriptive Properties
AppearanceFlakes
ColorWhite
Composition<0.004%Fluorides
 <0.004%Fluorides, Specifications
 <1 mg/kgHg
 <1 mg/kgHg, Specifications
 <1.5 g/kgCa(OH)2, Specifications
 <3 mg/kgAs
 <3 mg/kgAs, Specifications
 <40 g/kgMagnesium and alkali salts, Specifications
 <5 mg/kgPb, Specifications
 0.7 g/kgWater insoluble
 0.9 g/kgCa(OH)2
 1.02CaCl2.2H2 O
 1.6 g/kgSO4
 1.6 mg/kgPb
 10.2pH of 1:20 solution
 26 g/kgMagnesium and alkali salts
 26 g/kgNaCl
 4.5-11pH of 1:20 solution, Specifications
 4.7 mg/kgFe
 750-810 g/kgCaCl2, Specifications
 770 g/kgCaCl2
 99-107%CaCl2.2H2 O, Specifications
Granulometry1.4 percent<0.5 mm, statistical average
 1.8 percent<1.0 mm, statistical average
 100 percent<8.0 mm, typical value
 27 percent<2.0 mm, typical value
 49.3 percent<4.0 mm, statistical average
 5.5 percent<2.0 mm, statistical average
 6 percent<0.5 mm, typical value
 8 percent<1.0 mm, typical value
 83 percent<4.0 mm, typical value
 98.3 percent<8.0 mm, statistical average

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay Chemicals CASO® FEED FLAKES Calcium Chloride
Solvay Chemicals CASO® SIEVED FLAKES Calcium Chloride
Solvay Chemicals CASO® FOOD FLAKES Food additive E 509, Calcium Chloride
Solvay Chemicals CASO® FEED POWDER Calcium Chloride
Solvay Chemicals CASO® Granular Anhydrous Calcium Chloride >94%

WSOLV122 / 147771

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.