MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

CMW® 353 Copper Alloy  (discontinued **)
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: CMW® 353 material is an economical high strength, high conductivity copper base alloy. It is a heat treatable copper base alloy and its excellent properties are obtained largely through heat treatment. Its properties combine high hardness, strength and wear resistance with relatively high electrical and thermal conductivity.

CMW® 353 is superior in its combination of hardness and conductivity to such non-ferrous alloys as Yellow Brass, Gear Bronze, Manganese Bronze and Aluminum Bronze. Any current or heat conducting members in electrical or other machinery will, therefore, be improved when made of CMW® 353 material. High hardness, combined with the toughness which characterizes CMW® 353 material, gives it excellent wear resistance and makes it useful for flash welding dies, back up bars, bushings and current carrying bearings in combination with CMW®3 shafts.

Information provided by CMW Inc.

1

Key Words: UNS C18000 (Wrought)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.75 g/cc0.316 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 9090Castings
Tensile Strength, Ultimate 586 MPa85000 psiCastings
Tensile Strength, Yield 483 MPa70100 psiCastings
Elongation at Break 10 %10 %Castings
Reduction of Area 20 %20 %Castings
Modulus of Elasticity 114 GPa16500 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000359 ohm-cm0.00000359 ohm-cm48 % IACS
 
Thermal PropertiesMetricEnglishComments
CTE, linear 16.2 µm/m-°C
@Temperature 100 °C
9.00 µin/in-°F
@Temperature 212 °F
Thermal Conductivity 183 W/m-K1270 BTU-in/hr-ft²-°F
Melting Point 1038 - 1116 °C1900 - 2041 °F
Solidus 1038 °C1900 °F
Liquidus 1116 °C2041 °F
Softening Point 455 °C851 °FPermanent Softening
 
Component Elements PropertiesMetricEnglishComments
Chromium, Cr 0.80 %0.80 %
Copper, Cu 96.1 %96.1 %
Nickel, Ni 2.5 %2.5 %
Silicon, Si 0.60 %0.60 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Cadi MOLD-MOR™ 1
Cadi MOLD-MOR™ 10
IBC Advanced Alloys Thermal-Mould™ 180 C18000 Copper Chrome Silicon Nickel Alloy
MetalTek Copper Ni Si Cast UNS C81540 High Conductivity
ArcelorMittal IF 180 High strength IF steel, Cold rolled

NCMW069 / 15881

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.