MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik TEGO® Antifoam 1488 Emulsion
Categories: Other Engineering Material

Material Notes: Product description: TEGO® Antifoam 1488 is an antifoam emulsion based on organo-modified siloxanes.

Application: TEGO® Antifoam 1488 is used as antifoam in a broad range of aqueous based systems. It provides reliable foam control in water based adhesives as well as in the processing and appli-cation of polymer dispersions, emulsions and a multitude of other industrial applications, where the use of traditional silicone oil based antifoams is restricted for certain reasons. Applications for TEGO® Antifoam 1488 are:

  • Processing and application of polymer dispersions/ lattices
  • Textile industry (e.g. textile sizing, production of non-woven)
  • Tank side defoamer for all different types of aqueous metal working fluids (soluble oils, semi- and full synthetic fluids).
Properties / Benefits: TEGO® Antifoam 1488 has a unique product profile that combines excellent foam suppression and long term efficiency with maximum compatibility at the same time. These properties cannot be achieved with organic or with traditional silicone oil based antifoams. Furthermore undesirable effects associated with silicone based antifoams (silicone spotting, fish eyes) can be eliminated in most applications. TEGO® Antifoam 1488 is highly compatible. It does not deteriorate the shelf-life of ready-to-use emulsions.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.00 g/cc0.0361 lb/in³
pH 9.09.0
Viscosity 100 cP100 cP
 
Descriptive Properties
Appearancewhite emulsion
Content20%Active content

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik BREAK-THRU® AF 9908 Surfactants
Evonik SIPERNAT® 383 DS Silica Powder
Evonik TEGO® Antifoam 2-80 Emulsion
Evonik TEGO® Antifoam 3062 Antifoam concentrate
Evonik TEGOPREN® 5863 Defoamer

PEVONIL543 / 196747

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.