MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Huntsman IROGRAN® A 60 E 4902 TPU-Polyester
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: Introduction: IROGRAN A 60 E 4902 is a soft, high performance polyester based thermoplastic polyurethane intended for extrusion and molding applications. IROGRAN A 60 E 4902 is part of the HUNTSMAN Film and Sheet and Injection-Molding product ranges. It is processable at low temperatures and offers a specially designed, flexible material suitable for elastic films & moldings

Performance Features:

  • Excellent elasticity
  • Excellent wear performance
  • Good low temperature flexibility
  • Enhanced Hydrolytic Stability
  • Enhanced UV stability
  • Low temperature processability

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³Injection molded; ASTM D792
Melt Index of Compound 35 g/10 min
@Load 8.70 kg,
Temperature 160 °C
35 g/10 min
@Load 19.2 lb,
Temperature 320 °F
MVR
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5656Injection molded parts; ASTM D2240
Hardness, Shore D 1515Injection molded parts; ASTM D2240
Tensile Strength at Break 7.52 MPa1090 psi0.025" extruded film; ASTM D412
Elongation at Break 715 %715 %0.025" extruded film; ASTM D412
100% Modulus 1.40 MPa
@Strain 100 %
203 psi
@Strain 100 %
0.025" extruded film; DIN 53504
300% Modulus 2.40 MPa
@Strain 300 %
348 psi
@Strain 300 %
0.025" extruded film; DIN 53504
Rebound 60 %60 %Bayshore; ASTM D2632
Tear Strength 35.9 kN/m205 pli0.025" extruded film; ASTM D624
Abrasion 4343mm3, Injection molded; DIN 53516
Compression Set  40 %
@Temperature 22.8 °C,
Time 252000 sec
40 %
@Temperature 73.0 °F,
Time 70.0 hour
Injection molded; ASTM D395
 80 %
@Temperature 70.0 °C,
Time 86400 sec
80 %
@Temperature 158 °F,
Time 24.0 hour
Injection molded; ASTM D395
Tensile Set 8.0 %
@Strain 200 %
8.0 %
@Strain 200 %
0.025" extruded film; ASTM D412
 
Thermal PropertiesMetricEnglishComments
Melting Point 110 - 143 °C230 - 289 °F0.025" extruded film,
 
Processing PropertiesMetricEnglishComments
Feed Temperature 160 - 170 °C320 - 338 °F
Middle Barrel Temperature 160 - 170 °C320 - 338 °F
Nozzle Temperature 160 - 170 °C320 - 338 °F
Adapter Temperature 160 - 170 °C320 - 338 °F
Die Temperature 160 - 170 °C320 - 338 °F
Roll Temperature 115 °C239 °FFront
 115 °C239 °FRear

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Huntsman IROGRAN® A 70 E 4675 Polyester-Based TPU-High Performance Grade
BASF Elastollan® C-60AW Polyester Type Polyurethane Elastomer
Huntsman IROGRAN® A 60 E 4612 N TPU-Polyester
AlphaGary Vythene™ VYT/13E-55 CLEAR TL 0025 Polyurethane / Polyvinyl Chloride Compound
Covestro Texin® 5250 Thermoplastic Polyurethane, Polyether-based, Medical

PHUQ087 / 159460

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.