MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lubrizol LifeSciences Pellethane® 5863-87A TPU
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Ether Grade

Material Notes: Aromatic Polyether-based Thermoplastic Polyurethane (TPU)

Features: Good physical properties, hydrolysis resistance, low temperature performance and abrasion with a wide processing window for extrusion.

Process: Extrusion and Injection Molding.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.12 g/cc1.12 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8787ASTM D2240
Tensile Strength, Ultimate 51.7 MPa7500 psiASTM D412
Elongation at Break 500 %500 %ASTM D412
100% Modulus 6.90 MPa
@Strain 100 %
1000 psi
@Strain 100 %
ASTM D412
300% Modulus 12.4 MPa
@Strain 300 %
1800 psi
@Strain 300 %
ASTM D412
Tear Strength 26.3 kN/m150 pliTrouser; ASTM D470
Graves Tear Strength 87.7 kN/m500 plidie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 40
@Load 1.00 kg
40
@Load 2.20 lb
H-18; ASTM D3389
Tensile Set 18 %
@Temperature 200 °C
18 %
@Temperature 392 °F
ASTM D412
 
Thermal PropertiesMetricEnglishComments
Melting Point 150 °C302 °FKofler
 284 °C543 °F
Glass Transition Temp, Tg -45.0 °C-49.0 °F
 
Optical PropertiesMetricEnglishComments
Haze 1.0 %1.0 %pressed between glass; ASTM D1003
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 182 °C360 °FInjection Molding
Front Barrel Temperature 188 °C370 °FInjection Molding
Nozzle Temperature 193 °C379 °FInjection Molding
Zone 1 177 °C351 °FExtrusion
Zone 2 182 °C360 °FExtrusion
Zone 3 188 °C370 °FExtrusion
Zone 4 193 °C379 °FExtrusion
Adapter Temperature 193 °C379 °FExtrusion, 5
Die Temperature 193 °C379 °FExtrusion
 193 °C379 °FExtrusion, 2
Melt Temperature 193 °C379 °FInjection Molding
Mold Temperature 15.0 °C59.0 °FInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol Pellethane® 2363-80AE Thermoplastic Polyurethane Elastomer
Lubrizol LifeSciences Pellethane® 5863-82AE TPU
Lubrizol LifeSciences Pellethane® 5863-82A TPU
Lubrizol LifeSciences Pellethane® 2363-80AE TPU

PLUBR9037 / 203604

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.