MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Honeywell ACumist® P-20 PP homopolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Micronized polypropylene for matting, and non skid, or non slip applications for thick film industrial solvent coatings. Excellent abrasion resistance, used in powder coatings for matting and scratch resistance.

Information provided by Honeywell

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.910 g/cc0.0329 lb/in³
 
Chemical PropertiesMetricEnglishComments
Total Acid Number 0.000.00
 
Thermal PropertiesMetricEnglishComments
Dropping Point 145 °C293 °FMettler
 
Descriptive Properties
Hardness<0.5 dmmASTM D5
Product FormMicronized powder
Size, microns18-20

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient OnForce™ LFT PP-60LGF/001 Natural Polypropylene Homopolymer (PP Homopolymer)
Avient OnForce™ LFT PP-50LGF/001 Natural Polypropylene Homopolymer (PP Homopolymer)
Avient Maxxam™ PPR-40G Nat Polypropylene Homopolymer (PP Homopolymer)
Avient Maxxam™ PPH-40C Nat Polypropylene Homopolymer (PP Homopolymer)
Avient Maxxam™ PPH-30T Nat Polypropylene Homopolymer (PP Homopolymer)

PHONWL114 / 179659

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.