MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Epoxy Technology EPO-TEK® 305 Spectrally Transparent Epoxy
Categories: Polymer; Thermoset; Epoxy

Material Notes: Product Description: EPO-TEK® 305 is a two component, semi-rigid, optical grade epoxy for semiconductor packaging of fiber optics, optoelectronics and medical devices. It is an electrically and thermally insulating epoxy.

Advantages & Application Notes:

  • Capable of transmitting light in the UV range. %Transmission from 248 to 400 nm may be realized.
  • Tg and Shore D values are indicative of a somewhat “semi flexible or semi rigid” epoxy. It can be used for low stress applications in optics.
  • Low viscosity, water-like epoxy formulation. This allows for application by pouring, dip coating, brushing, or microdispensing methods.
  • Versatility in curing from 23°C to 80°C range. This allows many types of low cost plastic substrate or housings to be used.
  • Suggested applications:
    • Optics:
      • Index matching epoxy for adhesive and coating applications with Scientific / OEM instruments and sensor devices
      • LED potting and encapsulation; LCD glass-glass or glass-PET laminations
    • Fiber Optics: potting or sealing the fiber into the snout of the opto-package in order to provide stress relief.
    • PCB / General: low stress potting of electronics as a clear encapsulant, COB glob top encapsulant.

    Information Provided by Epoxy Technology

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.870 g/cc0.870 g/ccPart B
 1.25 g/cc1.25 g/ccPart A
Viscosity 150 - 250 cP
@Temperature 23.0 °C
150 - 250 cP
@Temperature 73.4 °F
100 rpm
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6666
Tensile Modulus 0.692 GPa100 ksiStorage
Shear Strength 13.0 MPa1880 psiLap
 >= 23.4 MPa>= 3400 psiDie
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 2.00e+13 ohm-cm<= 2.00e+13 ohm-cm
Dielectric Constant 4.46
@Frequency 1000 Hz
4.46
@Frequency 1000 Hz
Dissipation Factor 0.026
@Frequency 1000 Hz
0.026
@Frequency 1000 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 31.0 µm/m-°C17.2 µin/in-°FBelow Tg
 148 µm/m-°C82.2 µin/in-°FAbove Tg
Maximum Service Temperature, Air 100 °C212 °FContinuous
 200 °C392 °FIntermittent
Minimum Service Temperature, Air -55.0 °C-67.0 °FContinuous
 -55.0 °C-67.0 °FIntermittent
Glass Transition Temp, Tg >= 35.0 °C>= 95.0 °FDynamic Cure 20—200°C /ISO 25 Min; Ramp 10—200°C @ 20°C/Min
Decomposition Temperature 270 °C518 °FDegradation Temperature
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.4763
@Wavelength 589 nm
1.4763
@Wavelength 589 nm
uncured
Transmission, Visible  >= 91 %
@Wavelength 250 nm
>= 91 %
@Wavelength 250 nm
Spectral
 >= 97 %
@Wavelength 300 nm
>= 97 %
@Wavelength 300 nm
Spectral
 >= 98 %
@Wavelength 400 - 1600 nm
>= 98 %
@Wavelength 400 - 1600 nm
Spectral
 
Processing PropertiesMetricEnglishComments
Cure Time  60.0 min
@Temperature 65.0 °C
1.00 hour
@Temperature 149 °F
 1440 min
@Temperature 23.0 °C
24.0 hour
@Temperature 73.4 °F
Pot Life 60 min60 min
Shelf Life 12.0 Month
@Temperature 25.0 °C
12.0 Month
@Temperature 77.0 °F
 
Descriptive Properties
ColorClear/ColorlessPart A
 Clear/ColorlessPart B
ConsistencyPourable liquid
Mix Ratio by Weight100:2.8
Number of ComponentsTwo
Weight Loss1.22%200°C
 3.99%250°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AGC F-Clean® Clear
Epoxy Technology EPO-TEK® 301-2 Optically Transparent Epoxy
Epoxy Technology EPO-TEK® 301 Spectrally Transparent Epoxy
Tra-Con Tra-Bond F114 Optically Clear, Low Viscosity Blush-Free Epoxy Adhesive
Tra-Con Tra-Bond F202 Spectrally Transparent High Temperature Epoxy Adhesive

PPOXYT111 / 141150

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.