MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Saint-Gobain COHRlastic® F-12 Silicone Foam
Categories: Polymer; Thermoset; Silicone; Silicone Foam

Material Notes: Description: Low-density, flame-retardant COHRlastic silicone foam yard goods provide outstanding performance for industries ranging from aviation and mass transit to automotive, electronics, construction and furniture. In addition to a UL94V-O listing in thicknesses down to 1/16", it withstands a 2100°F flame for more than 10 minutes without burning through in thicknesses down to 3/8". The material, which has a nominal density of 12 pounds per cubic foot, generates very little white smoke. Non-corrosive for use with metals and in hostile environments, it has low compression set. Among its applications are fireblocks, thermal barriers, noie and vibration dampeners, insulationa dn high-performance gaskets or seals. For the aviation, automotive and mass transit industries, it offers a high degree of design flexibility. Lightweight and easy to process, it can be laminated to seat cover fabrics and carpeting as a backing for added flame resistance in passenger compartment furnishings. The material has similar uses in institutional and residential furnishings, marine and lighting applications. It offers properties valuable in flame retardant backings for floor, wall and furniture coverings; fire-wall and thermal barriers or insulation, padding and gasketing for commercial and private marine vehicles; or gasketing and sealing in high-intensity light fixtures and electronic components in medial, computer and business equipment. Supplied in 18" and 36" wide roll stock. Thicknesses are shown in the table below. It is available plain or, on special order, laminated to any of a wide range of substrates. Because of the unique nature of COHRlastic foam, SGPPL CHR has undertaken a rigorous testing program which is performed at outside independent laboratories. The tests document the flame resistant properties and low levels of toxicity and smoke generation as well as mechanical and electrical properties. Details are on file at SGPPL CHR.
  • Passes FDA Extractables, 21 CFR177.2600
  • Products Combustion (ASTM E662), Hydrogen Cyanide = 0 ppm
  • In compliance with Boston Fire Dept. Chair Test, January 1986
  • Passes FAR 25.853(a) and (b)
  • Passes UL94V-0
All data based on a 0.0625 inch test sample.(Other thicknesses available.)
Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.194 g/cc0.00700 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 0.172 MPa25.0 psi
Elongation at Break 60 %60 %
Compressive Strength 0.0207 MPa3.00 psiCompression Deflection, Compressed to 75% original thickness.; ASTM D1056
Compression Set 5.0 %
@Temperature 100 °C
5.0 %
@Temperature 212 °F
Constant Deflection, Compressed 50% for 22 hrs
 
Electrical PropertiesMetricEnglishComments
Insulation Resistance 2.30e+14 ohm2.30e+14 ohmASTM D257
 2.30e+14 ohm2.30e+14 ohmASTM D257
Dielectric Constant  1.3
@Frequency 1000 Hz
1.3
@Frequency 1000 Hz
ASTM D150
 1.31
@Frequency 100 Hz
1.31
@Frequency 100 Hz
ASTM D150
 1.32
@Frequency 1e+6 Hz
1.32
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 123 sec123 secASTM D495
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.0605 W/m-K0.420 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 204 °C400 °F
Minimum Service Temperature, Air -51.1 °C-60.0 °F
Flammability, UL94 V-0V-0
Flame Spread Index 11.511.5ASTM E162
 12.112.1Radiant Panel; ASTM D3675
Smoke Density 23 min23 min4 minutes, flaming mode; ASTM E662
 35 min35 min4 minutes, smoldering mode; ASTM E662
Oxygen Index 34 %34 %ASTM 2863
 
Descriptive Properties
ColorGray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Saint-Gobain COHRlastic® 512AF Silicone Foam/Acrylic Adhesive Pressure Sensitive Tape
Saint-Gobain COHRlastic® R10470 Medium General-Purpose Silicone Sponge Rubber
Rogers Corporation Bisco™ BF-1000 Cellular Silicone Foam
Armacell OleTex® BDJN 200 EVA/LDPE Foam
Evonik Rohacell® 31 Polymethacrylimide (PMI) Rigid Foam Sheet

PSTGQZ266 / 68780

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.