MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

Aluminum 6053-O
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 6000 Series Aluminum Alloy

Material Notes: Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN.

Composition Notes:
Composition information provided by the Aluminum Association and is not for design.

Key Words: UNS A96053; Aluminium 6053-O; AA6053-O; Al6053-O
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 2.69 g/cc0.0972 lb/in³AA; Typical
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 2626500 kg load with 10 mm ball
Tensile Strength, Ultimate 110 MPa16000 psi
Tensile Strength, Yield 55.0 MPa7980 psi
Elongation at Break 35 %
@Thickness 1.60 mm
35 %
@Thickness 0.0630 in
In 5 cm
Modulus of Elasticity 69.0 GPa10000 ksiAverage of Tension and Compression. In Al alloys, the compressive modulus is typically 2% greater than the tensile modulus. Estimated from trends in similar Al alloys.
Poissons Ratio 0.330.33Estimated from trends in similar Al alloys.
Fatigue Strength 55.0 MPa
@# of Cycles 5.00e+8
7980 psi
@# of Cycles 5.00e+8
Shear Modulus 26.0 GPa3770 ksiEstimated from similar Al alloys.
Shear Strength 75.0 MPa10900 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000382 ohm-cm
@Temperature 20.0 °C
0.00000382 ohm-cm
@Temperature 68.0 °F
AA; Typical
 
Thermal PropertiesMetricEnglishComments
CTE, linear  23.0 µm/m-°C
@Temperature 20.0 - 100 °C
12.8 µin/in-°F
@Temperature 68.0 - 212 °F
AA; Typical; average over range
 24.6 µm/m-°C
@Temperature 20.0 - 300 °C
13.7 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.890 J/g-°C0.213 BTU/lb-°FEstimated from trends in similar Al alloys.
Thermal Conductivity 171 W/m-K1190 BTU-in/hr-ft²-°FAA; Typical at 77°F
Melting Point 577 - 651.7 °C1070 - 1205 °FAA; Typical range based on typical composition for wrought products >= 1/4 in. thickness. Eutectic melting can be eliminated by homogenization.
Solidus 577 °C1070 °FAA; Typical
Liquidus 651.7 °C1205 °FAA; Typical
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 97.5 - 98.8 %97.5 - 98.8 %As remainder
Chromium, Cr 0.15 - 0.35 %0.15 - 0.35 %
Copper, Cu <= 0.10 %<= 0.10 %
Iron, Fe <= 0.35 %<= 0.35 %
Magnesium, Mg 1.1 - 1.4 %1.1 - 1.4 %
Other, each <= 0.05 %<= 0.05 %
Other, total <= 0.15 %<= 0.15 %
Zinc, Zn <= 0.10 %<= 0.10 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum 6053-T6
Aluminum 6005-T1
Aluminum 6061-O
Aluminum 6053-T4
Aluminum 6005-T5

MA6053O / 9378

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.