MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ATI Allegheny Ludlum Stainless Steel AL 904L™ Alloy (UNS N08904)
Categories: Metal; Ferrous Metal; Austenitic; Stainless Steel

Material Notes: Allegheny Ludlum AL 904 L™ Alloy (UNS N08904) is an austenitic stainless steel alloy designed for a middles to high level of corrosion resistance. The alloy is produced to low carbon levels for use in the welded condition as in welded vessels and other large and complex fabrications.

The high nickel (25%) and molybdenum (4.5%) contents of the AL 904L alloy provide good resistance to chloride stress corrosion cracking, although not total resistance as judged by the extremely severe laboratory test, boiling magnesium chloride.

The N08904 alloy has been incorporated in ASTM and ASME specifications, and is widely and readily available in a variety of product forms, welding electrodes, and fittings. The AL 904L Alloy has performed well in a variety of service environments such as utility scrubbers, acid and fertilizer production.

Information provided by Allegheny Ludlum Corporation.

Key Words: DIN 1.4539; ASTM B-625; ASME SB-625
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 7.90 g/cc0.285 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 150150Typical
Hardness, Rockwell B 70 - 9070 - 9079 Is Typical
Tensile Strength, Ultimate >= 490 MPa>= 71100 psi
 605 MPa87700 psiTypical
Tensile Strength, Yield >= 220 MPa>= 31900 psi
 270 MPa39200 psiTypical
Elongation at Break >= 36 %>= 36 %
 50 %50 %Typical
Reduction of Area 55 %55 %
Modulus of Elasticity 190 GPa27600 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000952 ohm-cm0.0000952 ohm-cm
Magnetic Permeability <= 1.02<= 1.02
 
Thermal PropertiesMetricEnglishComments
CTE, linear  15.3 µm/m-°C
@Temperature 20.0 - 100 °C
8.50 µin/in-°F
@Temperature 68.0 - 212 °F
 16.5 µm/m-°C
@Temperature 20.0 - 400 °C
9.17 µin/in-°F
@Temperature 68.0 - 752 °F
 18.2 µm/m-°C
@Temperature 20.0 - 800 °C
10.1 µin/in-°F
@Temperature 68.0 - 1470 °F
Specific Heat Capacity 0.460 J/g-°C0.110 BTU/lb-°Ftypical of N08904
Thermal Conductivity  11.5 W/m-K
@Temperature 20.0 °C
79.8 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
 12.9 W/m-K
@Temperature 100 °C
89.5 BTU-in/hr-ft²-°F
@Temperature 212 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.020 %<= 0.020 %
Chromium, Cr 19 - 23 %19 - 23 %
Copper, Cu 1.0 - 2.0 %1.0 - 2.0 %
Iron, Fe 47 %47 %as balance
Manganese, Mn <= 2.0 %<= 2.0 %
Molybdenum, Mo 4.0 - 5.0 %4.0 - 5.0 %
Nickel, Ni 23 - 28 %23 - 28 %
Phosphorus, P <= 0.045 %<= 0.045 %
Silicon, Si <= 1.0 %<= 1.0 %
Sulfur, S <= 0.035 %<= 0.035 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Outokumpu 904L High Performance Austenitic Stainless Steel
Carlson 904L Austenitic Stainless Steel
Type 904L Austenitic Stainless Steels, Annealed Bar, UNS N08904
420 Stainless Steel
Overview of materials for Nickel Alloy

NL904L / 17964

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.