MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mitsui LUCANT™ HC-600 Synthetic Oil
Categories: Fluid; Lubricant

Material Notes: LUCANT®, a hydrocarbon-based synthetic oil having no polar groups, is a co-oligomer of ethylene and -olefin. It possesses surpassing resistance to heat and cold and lower dependence of viscosity on temperature.

Characteristics
  • Non-volatile, colorless and transparent
  • Excellent viscosity-temperature properties
  • Low dependence of viscosity on temperature
  • Excellent heat and oxidation stability
  • Low pour point
  • High flash and fire points
  • Chemically stable, thus causing little or no metallic corrosion

Applications
  • Lubricant: Base oil and formulating ingredient for special lubricants, greases and functional fluids, which require resistance to heat and cold
  • Rubber: Oil extender and processability improver in cases, which require resistance to heat, cold and volatility
  • Resins: Softening and process agent
  • Other: Pressure-sensitive adhesive, bonding agents, coating materials, ink, heat medium and special solutions

Information provided by Mitsui Chemicals America, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.846 g/cc0.846 g/ccd204; Anton Paar density meter
Brookfield Viscosity  150000 cP
@Temperature 0.000 °C
150000 cP
@Temperature 32.0 °F
ASTM D2983
 400000 cP
@Temperature -10.0 °C
400000 cP
@Temperature 14.0 °F
ASTM D2983
 1.30e+6 cP
@Temperature -20.0 °C
1.30e+6 cP
@Temperature -4.00 °F
ASTM D2983
Viscosity Measurement 240240Viscosity Index; JIS K 2283
Kinematic Viscosity at 40°C (104°F) 9850 cSt9850 cStJIS K 2283
Kinematic Viscosity at 100°C (212°F) 600 cSt600 cStJIS K 2283
Ash <= 0.010 %<= 0.010 %JIS K 2272
ASTM Color 5.05.0ASTM D1209
 
Chemical PropertiesMetricEnglishComments
Acid Value <= 0.010<= 0.010[mg KOH/g]; total acid number; JIS K 2501
 
Thermal PropertiesMetricEnglishComments
Pour Point -15.0 °C5.00 °FJIS K 2269
Flammability Test 320320[°C]; Fire Point; JIS K 2265
 415415Autoignition temp.; ASTM D2155-66
Flash Point 302 °C576 °FCOC Method; JIS K 2265
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %transparent; thickness not quantified
 
Descriptive Properties
Aniline Point °CMin 170JIS K 2265
Carbon Residue wt%0.01JIS K 2270
Copper Corrosion1JIS K 2513
ReactionNeutralJIS K 2252

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mitsui LUCANT™ HC-10 Synthetic Oil
Mitsui LUCANT™ HC-2000 Synthetic Oil
Mitsui LUCANT™ HC-20 Synthetic Oil
Mitsui LUCANT™ HC-100 Synthetic Oil
Mitsui LUCANT™ HC-40 Synthetic Oil

PMIT123 / 53281

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.