MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

High-Leaded Tin Bronze, UNS C93600, Permanent Mold Cast M05
Categories: Metal; Nonferrous Metal; Copper Alloy; Copper Casting Alloy

Material Notes: Typically used for bearings and bushings. Good suitability for soldering and brazing. Not recommended for oxyacetylene, gas shielded, or coated metal welding.

Mechanical properties are for M05, as permanent mold cast.

Information provided by Spectrum Machine, Inc.

Key Words: MIL-C-22229 (sand cast)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 9.00 g/cc0.325 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 6565500 kg load
Tensile Strength, Ultimate 241 MPa35000 psiTypical
Tensile Strength, Yield 145 MPa
@Strain 0.5 %
21000 psi
@Strain 0.5 %
Typical
Elongation at Break 15 %15 %in 2 inches; Typical
Modulus of Elasticity 96.5 GPa14000 ksi
Machinability 80 %80 %Free Cutting Brass = 100%
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000156 ohm-cm0.0000156 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 18.5 µm/m-°C
@Temperature 20.0 - 200 °C
10.3 µin/in-°F
@Temperature 68.0 - 392 °F
Specific Heat Capacity 0.377 J/g-°C0.0900 BTU/lb-°F
Melting Point 843 - 938 °C1550 - 1720 °F
Solidus 843 °C1550 °F
Liquidus 938 °C1720 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 260 °C500 °FStress Relieving. Cannot be strengthened by heat treating.
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al <= 0.0050 %<= 0.0050 %
Antimony, Sb <= 0.55 %<= 0.55 %
Copper, Cu 79 - 83 %79 - 83 %Cu + sum of named elements 99.3% min.
Iron, Fe <= 0.20 %<= 0.20 %
Lead, Pb 11 - 13 %11 - 13 %
Nickel, Ni <= 1.0 %<= 1.0 %includes Co
Other, total <= 0.70 %<= 0.70 %
Phosphorus, P <= 0.15 %<= 0.15 %
Silicon, Si <= 0.0050 %<= 0.0050 %
Sulfur, S <= 0.080 %<= 0.080 %
Tin, Sn 6.0 - 8.0 %6.0 - 8.0 %
Zinc, Zn <= 1.0 %<= 1.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
High-Leaded Tin Bronze, UNS C93600, Centrifugal Cast M02
High-Leaded Tin Bronze, UNS C93600, Continuous Cast M07
High-Leaded Tin Bronze, UNS C93200, Copper Casting Alloy, Bearing Bronze SAE 660
High-Leaded Tin Bronze, UNS C93500, Copper Casting Alloy
High-Leaded Tin Bronze, UNS C93400, Copper Casting Alloy

MC93600b3 / 109232

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.