MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

M Chemical GUARD DOG™ UV328 Benzotriazole UV Absorber
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: GUARD DOG™ UV328 light stabilizer is a derivative of Benzotriazole that has exceptionally strong and broad-range UV absorption properties throughout the UV spectrum specially designed for polymers and coatings. Due to its extended UV absorption capability, this product provides excellent protection for plastics, top coats and various light sensitive substrates. It is highly recommended for thermoset plastics, organic substrates and coatings that function as weathering. This product may also be used in conjunction with other light stabilizers of HALS class to give plastics, coatings and paints superior protection against gloss reduction, cracking, color change, blistering, chalking and delamination. It is only recommended for room temperature and low temperature cured formulations such as air-dried alkyd or moisture cured PU based systems.

Applications: Guard Dog™ UV328 light stabilizer is recommended for applications such as automotive coatings, industrial coatings or wood stains. It is also recommended as a stabilizer for styrene homo- and copolymers, acrylic polymers, unsaturated polyesters, PVC, polyolefins, polyurethanes, polyacetals, polyvinylbutyral, elastomers and adhesives. The recommended dosage for plastics is less than 1% and for coatings between 1 - 3% depending on substrate and performance requirements.

Performance Benefits:

  • Strong and broad absorption of UV light in 270 - 380 nm range with low color contribution
  • High degree of inherent light stability and has low volatility
  • Excellent compatibility with polymers and exceptional UV protection for styrene, acrylic, PU, polyolefins, unsaturated polyesters, PVB and engineering polymers.

Typical Properties:

  • Pale yellow free flowing powder
  • Solubility (g/100g @ 25°C): MEK 14, Butanol 2.5, Ethylene Glycol 4, Butyl Acetate 15, Xylene 34, Mineral Spirit 14, Ethyl Acetate 20

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.910 g/cc
@Temperature 20.0 °C
0.910 g/cc
@Temperature 68.0 °F
Volatiles <= 0.50 %<= 0.50 %
Solubility in Water <= 0.010 %<= 0.010 %
Molecular Weight 351.5 g/mol351.5 g/mol
 
Thermal PropertiesMetricEnglishComments
Melting Point 80.0 - 88.0 °C176 - 190 °F
 
Descriptive Properties
Assay>99%by HPLC
CAS Number25973-55-1
Molecular FormulaC22H2911N3O
Name2-(2'-Hydroxy-3', 5'-di-t-amylphenyl) benzotriazole

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Addiplast Addilene J 490 M20F Flame Retardant Polypropylene, 20% Mineral Filled
M Chemical GUARD DOG™ UV234 Light Absorber, Benzotriazole Derivative
M Chemical GUARD DOG™ UV360 Light Absorber
M Chemical GUARD DOG™ UV531 Light Absorber (Flake or Powder), Benzophenone Derivative
M Chemical GUARD DOG™ UV123 HALS Light Stabilizer

PMCHEM907 / 135146

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.