MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Elastollan® 664 DU TPUR
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.

Typical Applications: Decorative parts and damping elements for the sport-shoe industry, ski tips, tubes and films.

Note: Quoted results are from measurements on injection molded test platens, post tempered for 20 hours at 100°C

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.23 g/cc0.0444 lb/in³ISO 1183-1-A
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6565ISO 686
Tensile Strength 40.0 MPa5800 psiISO 37
 40.0 MPa5800 psiafter storage in water at 80°C for 42 days; ISO 37
Tensile Stress at Strain  12.0 MPa
@Strain 20 %
1740 psi
@Strain 20 %
ISO 37
 20.0 MPa
@Strain 100 %
2900 psi
@Strain 100 %
ISO 37
Elongation at Break 350 %350 %ISO 37
 400 %400 %after storage in water at 80°C for 42 days; ISO 37
Charpy Impact, Notched  0.900 J/cm²
@Temperature -30.0 °C
4.28 ft-lb/in²
@Temperature -22.0 °F
DIN EN ISO 179
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
DIN EN ISO 179
Tear Strength 130 kN/m742 pliDIN ISO 34-1/Bb
Abrasion 3030[mm3; ISO 4649
Compression Set  35 %
@Temperature 23.0 °C
35 %
@Temperature 73.4 °F
ISO 815
 40 %
@Temperature 70.0 °C
40 %
@Temperature 158 °F
ISO 815
 
Processing PropertiesMetricEnglishComments
Processing Temperature 175 - 230 °C347 - 446 °FInjection molding
Mold Temperature 20.0 - 70.0 °C68.0 - 158 °F
 
Descriptive Properties
ColorTransparent
Commercial StatusNorth America
Primary Processing TechniqueInjection molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Elastollan® 690 AU TPUR
BASF Elastollan® 685 AU TPUR
BASF Elastollan® S 60 A SPF TPUR
BASF Elastollan® S 50 A SPF TPUR
BASF Elastollan® S 60 AWH TPUR

PBASG0510 / 132143

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.