MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Borealis HE1878E-C2 High Molecular Weight Polyethylene, Crosslinkable
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); UHMW PE (Ultra High Molecular Weight PE)

Material Notes: HE1878E-C2 is a high molecular weight, high density polyethylene specially designed for production of cross linked pipes (PE-X). HE1878E-C2 is recommended for the production of cross linked pipes used in plumbing, heating, district heating, relining, industrial, domestic gas, and domestic water.

Former trade name for this product was BorPEX™.

Information provided by Borealis AG

Key Words: XLPE;PEX
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.951 g/cc0.0344 lb/in³compound; ISO 1183
Oxidative Induction Time (OIT) >= 50 min
@Temperature 210 °C
>= 50 min
@Temperature 410 °F
EN 728
Melt Flow 10 g/10 min
@Load 21.6 kg,
Temperature 190 °C
10 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 22.0 MPa3190 psi50mm/min; ISO 527-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis HE1878E High Density Polyethylene Powder for Crosslinked Pipes
Borealis BorPEX™ HE2557 Yellow High Density Polyethylene Compound for Crosslinked Pipes (Pex-A (Peroxide))
Borealis HE2590 High Density Polyethylene Compound for Crosslinked Pipes (Pex-C (Irradiation))
Borealis HE2595 Black High Density Polyethylene Compound for Crosslinked Pipes (Pex-C (Irradiation))
Borealis HE1878 High Density Polyethylene Powder for Crosslinked Pipes

PBOREA340 / 108600

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.