MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M Scotchcast™ 2104 Electrical Insulating Resin
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Scotchcast 2104 Electrical Insulating Resin is a hard, two-part, polyurethane resin encapsulant designed especially for permanent splice protection. 2104 is formulated for many electrical applications requiring a hard, non-reenterable resin with good handling and performance characteristics. 2104 is also used as the insulating material for cable splices operating at 1000 volts or less and is rated for continuous use at 90°C with an overload rating 130°C. It may be stocked to cover all hard resin needs, ending the need for multiple encapsulant inventories. This resin is a two-part polyurethane, and is formulated with excellent wetting properties and low viscosity. 2104 flows well, even at low temperatures, filling the closure completely and eliminating voids. Cure time is fast; approximately one hour at 22°C and 20 hours at -4°C.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.03 g/cc0.0372 lb/in³
Moisture Absorption 0.280 %0.280 %7 days at RT
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7070ASTM D2240
Tensile Strength at Break 3.06 MPa444 psiASTM D412
Elongation at Break 98 %98 %ASTM D412
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 3.8
@Frequency 100 Hz,
Temperature 23.0 °C
3.8
@Frequency 100 Hz,
Temperature 73.4 °F
ASTM D150
Dielectric Strength 20.6 kV/mm524 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 90.0 °C194 °FContinuous
 130 °C266 °F
Glass Transition Temp, Tg -70.0 °C-94.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  60.0 min
@Temperature 21.0 °C
1.00 hour
@Temperature 69.8 °F
Option 1
 1200 min
@Temperature -4.00 °C
20.0 hour
@Temperature 24.8 °F
Option 2
Gel Time 18.0 min18.0 min
 
Descriptive Properties
AppearanceGreen

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M Scotchcast™ 2131 Flame-Retardant Compound
3M Scotchcast™ 5388 Electrical Epoxy Powder Resin
3M Scotchcast™ 262 Electrical Epoxy Powder Resin

PMM35241 / 169988

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.