MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Momentive Performance Materials RTV5222 White Adhesive Sealant, Low Modulus Paste
Categories: Polymer; Adhesive; Thermoset; Silicone; Silicone, RTV, Adhesive/Sealant Grade

Material Notes: One-part totally non-corrosive alkoxy cure. Alkoxy cure silicones are neutral cure materials that offer exceptional adhesion and are non-corrosive to most metals. Typical uses: Economical true neutral with primerless adhesion and long tooling time.

Data provided by the manufacturer, GE Silicones.

GE Silicones became a part of Momentive Performance Materials in 2006.

Key Words: RTV Silicones; R.T.V. Silicones
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.40 g/cc0.0506 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 2626
Tensile Strength, Ultimate 2.60 MPa377 psi
Elongation at Break 750 %750 %
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 3.9
@Frequency 60 Hz
3.9
@Frequency 60 Hz
Dielectric Strength 16.5 kV/mm419 kV/in
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 205 °C401 °FContinuous useful temperature.
Minimum Service Temperature, Air -60.0 °C-76.0 °FContinuous useful temperature.
 
Processing PropertiesMetricEnglishComments
Processing Temperature 25.0 °C77.0 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sika SikaFlex 219 LM Low Modulus Polyurethane Sealant
Momentive Performance Materials RTV122 White Adhesive Sealant, General Purpose Paste
Momentive Performance Materials RTV5223 Black Adhesive Sealant, Low Modulus Paste
Armstrong A-661 Epoxy Adhesive
Abatron AboCast/AboCure 8109-5

PZZGE914 / 40468

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.