MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

PBI Performance Products S26 Thermal Resistant Polybenzimidazole Solution
Categories: Fluid; Polymer; Thermoplastic; Polybenzimidazole (PBI)

Material Notes: Polybenzimidazole (PBI) solutions are suitable products for film casting, dip coating, spray coating and resin impregnation. PBI can be firmly adhered to steel, stainless steel, aluminum, copper, nickel- chromium, glass, ceramics and plastics. PBI coatings are highly resistant to heat and chemical attack. PBI will provide electrical insulation and wear resistance.
S26 is a solution containing nominally 26% w/w PBI solids in conjunction with 1.5% w/w LiCl salt in dimethylacetamide (DMAc) to  form a 2100 Poise solution. This grade is easily thinned and can be used for films or coatings.
The LiCl stabilizer imparts long shelf life and can be easily removed with an 85°C, 1-hour, aqueous wash of a thin film.

Information provided by PBI Performance Products

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 26.2 %26.2 %
Water Absorption 0.40 %
@Temperature 22.8 °C,
Time 86400 sec
0.40 %
@Temperature 73.0 °F,
Time 24.0 hour
for bulk PBI; ASTM D570
Viscosity 20 cP20 cP5% PBI Solids
 200 cP200 cP10% PBI Solids
 2000 cP2000 cP15% PBI Solids
 17500 cP17500 cP20% PBI Solids
 200000 cP200000 cP25% PBI Solids
 9000 - 11000 cP
@Temperature 100 °C
9000 - 11000 cP
@Temperature 212 °F
as supplied S26 solution
 190000 - 230000 cP
@Temperature 25.0 °C
190000 - 230000 cP
@Temperature 77.0 °F
as supplied S26 solution
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 160 MPa23200 psifor bulk PBI; ASTM D638
Elongation at Break 3.0 %3.0 %for bulk PBI
Tensile Modulus 5.90 GPa856 ksifor bulk PBI
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 3.4
@Frequency 1000 Hz
3.4
@Frequency 1000 Hz
for bulk PBI; ASTM D150
Dielectric Strength 23.0 kV/mm584 kV/infor bulk PBI; ASTM D149
Dissipation Factor 0.0030
@Frequency 10000 Hz
0.0030
@Frequency 10000 Hz
for bulk PBI; ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 23.0 µm/m-°C
@Temperature 25.0 - 150 °C
12.8 µin/in-°F
@Temperature 77.0 - 302 °F
for bulk PBI; ASTM TMA
Glass Transition Temp, Tg 427 °C801 °Ffor bulk PBI; ASTM DMA
 
Processing PropertiesMetricEnglishComments
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
Colorred-brown
LiCl %1.5
Solvent (DMAc) %72.3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Elkem (Bluestar Silicones) BLUESIL™ FLD 47 V 3 Polydimethylsiloxanic Fluids
Syensqo (Solvay Specialty Polymers) Galden® DET PFPE Fluid
Paratherm Corporation Paratherm™ NF Heat Transfer Fluid
PBI Performance Products Celazole® TF-60 C Carbon Fiber Reinforced Melt Processable Polybenzimidazole
PBI Performance Products Celazole® TU-60 Unreinforced Melt Processable Polybenzimidazole

PPBIP006 / 140560

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.