MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

Markforged HSHT FG 3D Printed Composite
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic

Material Notes: High Strength High Temperature (HSHT) Fiberglass is best used for parts loaded in high operating temperatures. Continuous Filament Fabrication (CFF) adds fiber reinforcement to printed parts. Within a thermoplastic matrix, Markforged uses proprietary technology to lay down continuous long-strand fiber. Users can control the layers reinforced, amount, orientation, and type of reinforcing fiber.

Information provided by Markforged, Inc.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.50 g/cc0.0542 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 600 MPa87000 psiASTM D638
Elongation at Break 3.9 %3.9 %ASTM D638
Tensile Modulus 21.0 GPa3050 ksiASTM D638
Flexural Strength 420 MPa60900 psiASTM D790
Flexural Modulus 21.0 GPa3050 ksiASTM D790
Flexural Strain at Break 2.2 %2.2 %ASTM D790
Compressive Strength 192 MPa27800 psiASTM D6641
Compressive Modulus 21.0 GPa3050 ksiASTM D6641
Izod Impact, Notched 31.0 J/cm58.1 ft-lb/inASTM D256-10A
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 150 °C302 °FDeflection Temperature; load unknown; ASTM D648B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Markforged Fiberglass 3D Printed Composite
Markforged Carbon 3D Printed Composite
Markforged Nylon 3D Printed Polymer
Markforged Onyx 3D Printed Nylon Carbon Composite
Markforged Kevlar® 3D Printed Composite

PMARKF995 / 230540

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.