MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Adamas Rixon 130 PEEK, 30% Carbon Filled
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Carbon Fiber Filled

Material Notes:

Information provided by Adamas, HPM

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.41 - 1.44 g/cc1.41 - 1.44 g/ccASTM D792
Water Absorption 0.15 - 0.18 %0.15 - 0.18 %Immersion 24 hrs; ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 93 - 9593 - 95ASTM D785
Hardness, Shore D 85 - 9085 - 90ASTM D2240
Ball Indentation Hardness 330 - 350 MPa47900 - 50800 psiISO 2032-N961
Tensile Strength at Break 110 - 140 MPa16000 - 20300 psiASTM D638
Elongation at Break 2.0 - 4.0 %2.0 - 4.0 %ASTM D638
Tensile Modulus 1.00 - 1.10 GPa145 - 160 ksiASTM D638
Flexural Strength 200 - 220 MPa29000 - 31900 psi3.5% flexural stress; ASTM D4894
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+6 ohm-cm1.00e+6 ohm-cmASTM D257
Surface Resistance 1e+051e+05ASTM D257
 
Thermal PropertiesMetricEnglishComments
Melting Point 343 °C649 °FDSC
Maximum Service Temperature, Air 250 °C482 °FDSC
Minimum Service Temperature, Air -80.0 °C-112 °FDSC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Adamas Rixon 430 PEEK, 30% Carbon Fiber
Clariant Renol PA111G20CF10BK Nylon 66, 20% Glass and 10% Carbon Filled
Gharda Chemicals GATONE™ PEEK, 30% Carbon Fiber Reinforced
Ensinger Tecapeek® XP-101 Compression Molded PEEK Compound, Filled with 15% Graphite and 10% PTFE
Ensinger Tecapeek® XP-102 Compression Molded PEEK Compound, Filled with 15% Graphite and 10% PTFE

PHADAM001 / 147194

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.