MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Copper, UNS C62300 (Aluminum Bronze 9%), H50 Temper 25-50 mm rod
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: Good to excellent corrosion resistance. Good hot and cold formability. Fabricated by bending, hot pressing, forming, and welding.

Applications: bearings, bushings, valve guides, gears, valve seats, nuts, bolts, pump rods, work gears, and cams.

Test specimen: rod - 25-50mm diameter.

Key Words: CDA 623, CA106, ISO CuAl8Fe3
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 7.65 g/cc0.276 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 8989
Tensile Strength, Ultimate 605 MPa87700 psi
Tensile Strength, Yield 305 MPa44200 psiDepending on temper
Elongation at Break 15 %15 %in 50 mm, 15% reduction in area
Modulus of Elasticity 115 GPa16700 ksi
Compressive Yield Strength 345 MPa50000 psiAt permanent set of 0.1%
 448 MPa65000 psiAt permanent set of 1%
 676 MPa98000 psiAt permanent set of 10%
 931 MPa135000 psiAt permanent set of 20%
Poissons Ratio 0.3280.328
Fatigue Strength 200 MPa
@# of Cycles 1.00e+8
29000 psi
@# of Cycles 1.00e+8
Reverse Bending; Temper Not Reported
Machinability 50 %50 %
Forgeability 75 %75 %
Shear Modulus 44.0 GPa6380 ksi
Izod Impact 43.0 - 47.0 J31.7 - 34.7 ft-lbTemper not specified
Charpy Impact 25.0 - 40.0 J18.4 - 29.5 ft-lbV-notch
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000144 ohm-cm
@Temperature 20.0 °C
0.0000144 ohm-cm
@Temperature 68.0 °F
Magnetic Permeability 1.171.17
 
Thermal PropertiesMetricEnglishComments
CTE, linear 16.2 µm/m-°C
@Temperature 20.0 - 300 °C
9.00 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.375 J/g-°C0.0896 BTU/lb-°F
Thermal Conductivity 54.4 W/m-K
@Temperature 20.0 °C
378 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point 1040 - 1045 °C1900 - 1913 °F
Solidus 1040 °C1900 °F
Liquidus 1045 °C1913 °F
Annealing Point 593 - 649 °C1100 - 1200 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 1010 °C1850 °FHot-Shortness Temperature
Annealing Temperature 600 - 650 °C1110 - 1200 °F
Hot-Working Temperature 700 - 875 °C1290 - 1610 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 8.5 - 11 %8.5 - 11 %
Copper, Cu 82.2 - 89.5 %82.2 - 89.5 %
Iron, Fe 2.0 - 4.0 %2.0 - 4.0 %
Manganese, Mn <= 0.50 %<= 0.50 %
Other, total <= 0.50 %<= 0.50 %
Silicon, Si <= 0.25 %<= 0.25 %
Tin, Sn <= 0.60 %<= 0.60 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Copper, UNS C62300 (Aluminum Bronze 9%), Cold Finished Rod
Copper, UNS C62300 (Aluminum Bronze 9%)
Copper, UNS C62300 (Aluminum Bronze 9%), Annealed Rod
Copper, UNS C62300 (Aluminum Bronze 9%), H50 Temper, 25 mm rod
Aluminum Bronze, 5%, UNS C60600, H04 Temper

MC62300b3 / 11604

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.