MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SunChemical Gwent C2040308D2 Silver/Silver Chloride Paste
Categories: Fluid; Metal; Other Engineering Material; Ceramic/Metallic Coating

Material Notes: Silver/Silver Chloride Paste has a ratio of Silver to Silver Chloride of 40/60. The paste is in a ready to use form at a viscosity suitable for automatic or semi-automatic screen printing. The paste should be gently stirred before use avoiding introduction of air bubbles.
Applications in medical diagnostics, environmental sensor and the ’agri-food’ industries
Screen Printing Equipment: semi-automatic, manual
Screen Types: polyester, mesh 156-325tpi
Substrate: Polyester, PVC, Polycarbonate or ceramic. Note: Stainless steel mesh is not recommended, since a paste component can become corrosive in the presence of moisture. Also, plastic palette knives should be used instead of metal knives.

Information provided by Gwent Electronic Materials Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 81.14 - 83.14 %
@Temperature 130 °C
81.14 - 83.14 %
@Temperature 266 °F
Viscosity 3500 - 7000 cP
@Shear Rate 230 1/s,
Temperature 25.0 °C
3500 - 7000 cP
@Shear Rate 230 1/s,
Temperature 77.0 °F
Haake VT 550 PK1.1°
Thickness 28.0 microns1.10 milUsing a 230 mesh stainless steel screen, 13 micron emulsion
Storage Temperature 20.0 °C68.0 °Fsealed container
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 0.64 ohm
@Thickness 0.0280 mm
0.64 ohm
@Thickness 0.00110 in
Printed through 230 stainless steel mesh with 13 micron emulsion
 
Processing PropertiesMetricEnglishComments
Cure Time  10.0 min
@Temperature 80.0 °C
0.167 hour
@Temperature 176 °F
 30.0 min
@Temperature 60.0 °C
0.500 hour
@Temperature 140 °F
Shelf Life 3.00 Month3.00 Month
 
Descriptive Properties
Conductive Filler TypeSilver (Ag) / Silver Chloride (AgCl)
Coverage cm2/g130Using a 230 mesh stainless steel screen
Material TypeReady-To-Use Formulation
Recommended SubstratesPolyester, PVC, Polycarbonate or ceramic
Solvent SystemEthoxy Propanol or Sericol

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
SunChemical Gwent C2051014P10 Silver/Silver Chloride Paste
SunChemical Gwent C2030812D3 Silver/Silver Chloride Paste

WGELZ9020 / 139333

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.