MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Fortron® 4665 B6 Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled

Material Notes: Mineral/glass-fiber, excellent flow, high Comparative Tracking Index (electrical)

Information provided by Celanese Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.00 g/cc0.0723 lb/in³ASTM D792
Water Absorption 0.020 %0.020 %ASTM D570
Linear Mold Shrinkage, Flow 0.0015 cm/cm0.0015 in/in
Linear Mold Shrinkage, Transverse 0.0040 cm/cm0.0040 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 100100ASTM D785
Tensile Strength, Ultimate 104 MPa15100 psiASTM D638
Elongation at Break 1.3 %1.3 %ASTM D638
Flexural Strength 176 MPa25500 psiASTM D790
Flexural Modulus 16.5 GPa2390 ksiASTM D790
Izod Impact, Notched 0.400 J/cm0.749 ft-lb/inASTM D256
Izod Impact, Unnotched 2.10 J/cm3.93 ft-lb/inASTM D4812
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmASTM D257
Dielectric Constant  4.4
@Frequency 1e+6 Hz
4.4
@Frequency 1e+6 Hz
ASTM D150
 4.5
@Frequency 1000 Hz
4.5
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 12.0 kV/mm
@Thickness 3.17 mm
305 kV/in
@Thickness 0.125 in
ASTM D149
Dissipation Factor  0.0010
@Frequency 1e+6 Hz
0.0010
@Frequency 1e+6 Hz
ASTM D150
 0.0067
@Frequency 1000 Hz
0.0067
@Frequency 1000 Hz
ASTM D150
Arc Resistance 185 sec185 secASTM D495
Comparative Tracking Index 250 V250 VUL746A
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  19.0 µm/m-°C
@Temperature 20.0 °C
10.6 µin/in-°F
@Temperature 68.0 °F
ASTM D696
 35.0 µm/m-°C
@Temperature 100 °C
19.4 µin/in-°F
@Temperature 212 °F
ASTM D696
CTE, linear, Transverse to Flow  24.0 µm/m-°C
@Temperature 20.0 °C
13.3 µin/in-°F
@Temperature 68.0 °F
ASTM D696
 75.0 µm/m-°C
@Temperature 100 °C
41.7 µin/in-°F
@Temperature 212 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 280 °C536 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 260 °C500 °FASTM D648
UL RTI, Electrical 220 °C428 °F
UL RTI, Mechanical with Impact 200 °C392 °F
UL RTI, Mechanical without Impact 220 °C428 °F
Flammability, UL94 V-0
@Thickness 0.790 mm
V-0
@Thickness 0.0311 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese FORTRON 4184L4 PPS, 53% Mineral / Glass Reinforced
Celanese Fortron® 6165 A4 Polyphenylene Sulfide (PPS), 65% Mineral/Glass-Fiber
Celanese Fortron® 1140 L6 Polyphenylene Sulfide (PPS), 40% Glass Fiber
Celanese Fortron® 1140 L7 Polyphenylene Sulfide (PPS), 40% Glass Fiber
Celanese Fortron® 4184 L4 Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled

PHCU24 / 45764

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.