MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Boron Chloride, BCl3
Categories: Ceramic; Halide; Fluid

Material Notes: CAS Number: 10294-34-5

Physical Form: Colorless Liquid or Gas

Key Words: BCl3
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 4.789 g/cc0.1730 lb/in³Liquid
Molecular Weight 117.169 g/mol117.169 g/mol
 
Chemical PropertiesMetricEnglishComments
Critical Pressure 38.7000 bar29027.4 torr
Critical Temperature 182 °C360 °F
Critical Molar Volume 239 cm³/mol14.6 in³/mol
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 17.92 J/g7.710 BTU/lb
Heat of Vaporization 202.9 J/g87.27 BTU/lbAt Boiling Point
Specific Heat Capacity 0.5351 J/g-°C0.1279 BTU/lb-°FGas
 0.9107 J/g-°C0.2177 BTU/lb-°FLiquid
Melting Point -107 °C-161 °F
Boiling Point 12.65 °C54.77 °F
Heat of Formation -427.3 kJ/mol-427.3 kJ/molLiquid
 -403.8 kJ/mol-403.8 kJ/molGas
 
Descriptive Properties
SolubilityReacts with H2O and EtOH

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hydrogen Bromide, HBr
Bromine Trifluorine, BrF3
Bromine Pentafluoride, BrF5
Boron Trifluoride, BF3
Boron Trichloride, BCl3

EINOR2264 / 4398

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.