Product Description: LL 6100 is a narrow molecular weight butane copolymer designed for applications that require easy processability. This resin offers outstanding toughness and tear resistance in freezer applications for food packaging. Availability: Latin America, North America and South America Applications: - Closures and Dispensers
- Housewares
- Protective Caps
Information provided by ExxonMobil Chemical |