MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Arkema Kynar® ADX 281 PVDF
Material Notes:

Information provided by Arkema.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.77 g/cc0.0639 lb/in³ISO 1183
Water Absorption 0.10 %0.10 %Dry; Sim. to ISO 62
Moisture Absorption 0.0600 %0.0600 %Dry; Sim. to ISO 62
Melt Flow 25 g/10 min
@Load 5.00 kg,
Temperature 230 °C
25 g/10 min
@Load 11.0 lb,
Temperature 446 °F
cm³/10 min Volumetric Rate; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 42.0 MPa6090 psiDry; ISO 527-1/-2
Elongation at Break 46 %46 %Dry; ISO 527-1/-2
Elongation at Yield 10 %10 %Dry; ISO 527-1/-2
Tensile Modulus 1.50 GPa218 ksiDry; ISO 527-1/-2
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.00e+14 ohm-cm2.00e+14 ohm-cmDry; IEC 60093
Surface Resistance 1.00e+13 ohm1.00e+13 ohmCond.; IEC 60093
Dielectric Constant  6.5
@Frequency 1e+6 Hz
6.5
@Frequency 1e+6 Hz
Dry; IEC 60250
 10.5
@Frequency 100 Hz
10.5
@Frequency 100 Hz
Dry; IEC 60250
Dielectric Strength 21.0 kV/mm533 kV/inDry; IEC 60243-1
Dissipation Factor  0.038
@Frequency 100 Hz
0.038
@Frequency 100 Hz
Dry; IEC 60250
 0.234
@Frequency 1e+6 Hz
0.234
@Frequency 1e+6 Hz
Dry; IEC 60250
Comparative Tracking Index 600 V600 VDry; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 157 °C315 °F10°C/min; Dry; ISO 11357-1/-3
Glass Transition Temp, Tg -40.0 °C-40.0 °F10°C/min; Dry; ISO 11357-1/-2
 
Descriptive Properties
Form as DeliveredPowder
Heat StabilizedYes
Light StabilizedYes
Moisture SensitiveNo
Processing MethodsCoating

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Arkema Kynar® ADX 111 PVDF
Arkema Kynar® ADX 1720-03 PVDF
VICTREX™ PEEK 450G™ General Purpose
Arkema Kynar® ADX 1285-03 PVDF
Evonik Trogamid® T5000 Nylon 6-3

PARKF746 / 193538

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.