MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Esenttia 01R25 Random Copolymer Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Characteristics: Low melt flow rate high ethylene level Random copolymer polypropylene, very good impact.

Recommended for: Extrusion blow molding containers; co-extruded blown films; extrusion of strapping, Cartonplast; sheet extrusion and Solid Pressure Phase Forming of containers that require clarity and very good impact resistance, pure or blended with homopolymer.

Information provided by Esenttia by Propilco

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow 0.80 g/10 min
@Load 2.16 kg,
Temperature 230 °C
0.80 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238B
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 24.13 MPa3500 psi50 mm/min; ASTM D638
Elongation at Yield 13.5 %13.5 %50 mm/min; ASTM D638
Flexural Modulus, 1% Secant 792.9 MPa115000 psi1.3 mm/min; ASTM D790-1A
Izod Impact, Notched 1.2811 J/cm2.4000 ft-lb/inASTM D256-A
Gardner Impact 30.51 J22.50 ft-lbASTM D5420A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Esenttia 16C12NA Impact Block Copolymer Polypropylene
Esenttia 01R25-T Random Copolymer Polypropylene
Esenttia 01C25 Impact Block Copolymer Polypropylene

PESEN028 / 184600

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.