MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

ExxonMobil Bicor™ 70 MB OPP Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Product Description: Bicor 70 MB is a biaxially oriented polypropylene film for use in metalized film applications. 70 MB, when metalized, is used in adhesive and extrusion laminations to reveres-printed outer webs. Metalized 70 MB has outstanding moisture and light barrier. The proprietary broad seal range layer offers excellent hot tack, seal integrity, and lap seal range when used with a coextruder outer web.

Availability: North America and South America

Key Features:

  • Low MST, broad seal range, strong seals
  • High Adhesion of aluminum to film
  • Resists crazing in extrusion lamintations
Applications:
  • Bakery
  • Biscuits/Cookie/Crackers
  • Crisps and Snacks
  • Frozen Food
  • Ice Cream
Uses:
  • HFFS Flexible Packaging
  • Pre-made Bags-Flexible Packaging
  • VFFS Flexible Packaging
Processing Method: Inner Web Adhesive Lamination, Inner Web Extrusion Lamination, Solvent Flexographic Printing, Solvent Rotogravure Printing, Surface Print Unsupported and Water-based Flexographic Printing

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 17.8 microns0.700 milExxonMobil Method
Coating Weight 15.7 g/m²9.80 lb/reamExxonMobil Method
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 160 %160 %20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
Film Elongation at Break, TD 50 %50 %20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
Coefficient of Friction 0.550.55Treated; ExxonMobil Method
 0.700.70Untreated; ExxonMobil Method
Film Tensile Strength at Break, MD 138 MPa20000 psi20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
Film Tensile Strength at Break, TD 256 MPa37100 psi20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
 
Thermal PropertiesMetricEnglishComments
Shrinkage, MD 3.0 %
@Temperature 135 °C
3.0 %
@Temperature 275 °F
ExxonMobil Method
Shrinkage, TD 4.0 %
@Temperature 135 °C
4.0 %
@Temperature 275 °F
ExxonMobil Method
 
Optical PropertiesMetricEnglishComments
Haze 2.4 %2.4 %ExxonMobil Method
Gloss 86 %86 %45°, Untreated Surface; ExxonMobil Method
 
Descriptive Properties
Crimp Seal MST88°C
Crimp Seal Strength440 g/inUntreated/Untreated, 205°F (96°C), 20 psi (0.1 MPa), 0.8 sec
Yield44000 in2/lb

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil Bicor™ 15MB440 OPP Film
ExxonMobil Bicor™ 120 XRG-2 OPP Film
ExxonMobil Bicor™ 21MB777 OPP Film
Flint Hills 44S2A Polypropylene Impact Copolymer
ExxonMobil Bicor™ 70 XRG-2 OPP Film

PEX99458 / 175694

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.