MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Bayblend® FR421 MT PC Blend
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Unreinforced, Flame Retardant

Material Notes: Rubber modified PC blend; mineral filled ; flame retardant; Vicat/B 120 temperature = 134 °C; extrusion grade for aircraft interiors

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.29 g/cc0.0466 lb/in³ISO 1183-1
Moisture Absorption at Equilibrium 0.20 %0.20 %ISO 62
Water Absorption at Saturation 0.50 %0.50 %ISO 62
Viscosity 640000 cP
@Frequency 1000 Hz,
Temperature 260 °C
640000 cP
@Frequency 1000 Hz,
Temperature 500 °F
Melt; b.o. ISO 11443-A
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/in150x105x3 mm; 260 °C / MT 80 °C; b. o. ISO 2577
Linear Mold Shrinkage, Transverse 0.0060 - 0.0080 cm/cm0.0060 - 0.0080 in/in150x105x3 mm; 260 °C / MT 80 °C; b. o. ISO 2577
Melt Flow 2.58 g/10 min
@Load 5.00 kg,
Temperature 260 °C
2.58 g/10 min
@Load 11.0 lb,
Temperature 500 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 47.0 MPa6820 psi50 mm/min; ISO 527-1,-2
Tensile Strength, Yield 58.0 MPa8410 psi50 mm/min; ISO 527-1,-2
Elongation at Break 22 %22 %50 mm/min; ISO 527-1,-2
Elongation at Yield 4.0 %4.0 %50 mm/min; ISO 527-1,-2
Tensile Modulus 3.40 GPa493 ksi1 mm/min; ISO 527-1,-2
Izod Impact, Notched (ISO) 30.0 kJ/m²14.3 ft-lb/in²ISO 180-A
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmIEC 60093
Surface Resistance 1.00e+16 ohm1.00e+16 ohmIEC 60093
Dielectric Constant  3.0
@Frequency 1e+6 Hz
3.0
@Frequency 1e+6 Hz
IEC 60250
 3.1
@Frequency 100 Hz
3.1
@Frequency 100 Hz
IEC 60250
Dielectric Strength 41.0 kV/mm
@Thickness 1.00 mm
1040 kV/in
@Thickness 0.0394 in
IEC 60243-1
Dissipation Factor  0.0046
@Frequency 100 Hz
0.0046
@Frequency 100 Hz
IEC 60250
 0.0094
@Frequency 1e+6 Hz
0.0094
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 200 V200 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 50.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
27.8 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1, -2
CTE, linear, Transverse to Flow 60.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
33.3 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1, -2
Deflection Temperature at 0.46 MPa (66 psi) 129 °C264 °FISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 118 °C244 °FISO 75-1,-2
Vicat Softening Point  132 °C
@Load 5.10 kg
270 °F
@Load 11.2 lb
50°C/h; ISO 306
 134 °C
@Load 5.10 kg
273 °F
@Load 11.2 lb
120°C/h; ISO 306
Flammability, UL94  V-0
@Thickness 0.750 mm
V-0
@Thickness 0.0295 in
 5VA
@Thickness 3.00 mm
5VA
@Thickness 0.118 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 °C500 °FInjection; ISO 294
Mold Temperature 80.0 °C176 °FInjection; ISO 294
Injection Velocity 240 mm/sec9.45 in/secISO 294

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Bayblend® FR411 MT PC Blend
Covestro Bayblend® FR1514 PC/ABS Blend
Covestro Bayblend® CG100 PC/ABS Blend

PCOVEST0043 / 201826

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.