MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

A. Schulman Diamond Softflex® SF 5591 Thermoplastic Vulcanizate (TPV)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes:

A. Schulman has acquired Network Polymers & Diamond Polymers.

Key Words: Thermoplastic Elastomer Alloy
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.910 g/cc0.0329 lb/in³ASTM D792
Linear Mold Shrinkage, Flow 0.027 - 0.029 cm/cm
@Thickness 3.17 mm
0.027 - 0.029 in/in
@Thickness 0.125 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 3.20 MPa464 psichs 2.0 in/min; ASTM D638
Elongation at Break 415 %415 %chs 2.0 in/min; ASTM D638
Compression Set 30 %
@Temperature 25.0 °C,
Time 79200 sec
30 %
@Temperature 77.0 °F,
Time 22.0 hour
ASTM D395
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94 HB
@Thickness 1.47 mm
HB
@Thickness 0.0580 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman Diamond Softflex® SF 7001 Thermoplastic Vulcanizate (TPV)
Alliance Polymers Viprene™ G40D-32U-BLK Thermoplastic Vulcanizate Elastomer
Teknor Apex Sarlink® 3190 Thermoplastic Elastomer
Chengdu Polyster 9500 General Grade TPV
ExxonMobil Santoprene® 8123-45S100 Thermoplastic Elastomer

PDIAM496 / 126587

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.